HDPE DOW™ DMDH-6400 DOW USA
43
- Unit Price:US$ 1,457 /MT
- Packaging Specification:
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:characteristic:|Has strong glossiness|two|High impact resistance|three|Superior tensile strength performance
- Application Areas:--
- Color:--
- Grade:Blow molding grade
Technical Data Sheet
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Environmental stress cracking resistance | 122oF(50℃),F50,100%lgepal | ASTM D-1693 | 20 hrs |
Basic Performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | @190℃/2.16kg | ASTM D-1238 | 0.80 g/10min |
@190℃/21.60kg | ASTM D-1238 | 57 g/10min | |
density | ASTM D-792 | 0.961 g/cm³ |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ASTM D-2240 | 66 Shore D | |
tensile strength | Break | ASTM D-638 | 3500(24) Psi(MPa) |
Bending modulus | 2%割线 | ASTM D-790B | 188.000(1296) Psi(MPa) |
elongation at yield | ASTM D-638 | 7 % | |
Impact strength of cantilever beam gap | ASTM D-1822 | 40(84) ft·lb/in.2(KJ/m2) | |
elongation | Break | ASTM D-638 | 1000 % |
tensile strength | Yield | ASTM D-638 | 4600(32) Psi(MPa) |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Crystallization peak temperature | Dow Method | 248(120) oF(℃) | |
Vicat softening temperature | ASTM D-1525 | 268(131) oF(℃) | |
Melting temperature | Dow Method | 271(133) oF(℃) | |
Hot deformation temperature | @66psi(0.45MPa) | ASTM D-648 | 169(76) oF(℃) |
Brittle temperature | ASTM D-746 | <-105(<-76) oF(℃) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.