PC 1809-01 SHANDONG LUXI CHEM
208
- Unit Price:US$ 1,557 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:95MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 1.80MPa,4.0mm | ISO 75 | 127 °C |
vicat | B120, 4.0mm | ISO 306 | 148 °C |
flammability | 1.5mm | UL 94 | HB |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
transmittance | 3.2mm | ASTM D1003 | 90 % |
haze | 3.2mm | ASTM D1003 | <0.5 % |
Yellowness Index | 380-780nm | ISO 17223 | <2 |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | 300℃,1.2kg | ISO 1133 | 9 g/10min |
density | ISO 1183 | 1.2 g/cm³ | |
water absorption rate | 23℃,24h | ISO 62 | 0.2 % |
shrinkage rate | MD | ISO 294 | 0.5-0.7 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
volume resistivity | 5min | IEC 60093 | 300000000000000000 ohms·cm |
dielectric constant | IEC 60250 | 2.7 1 MHz | |
dielectric strength | 1mm | IEC 60243 | 30 KV/mm |
Dissipation Factor | IEC 60250 | 150 1 MHz |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | 屈服50mm/min | ISO 527 | 60 Mpa |
断裂50mm/min | ISO 527 | 70 Mpa | |
Tensile strain | 50mm/min | ISO 527 | >120 % |
tensile modulus | 1mm/min | ISO 527 | 2400 Mpa |
bending strength | 2mm/min | ISO 178 | 90 Mpa |
flexural modulus | 2mm/min | ISO 178 | 2300 Mpa |
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23℃ | ISO 179 | 72 kJ/m² |
Impact strength of cantilever beam gap | 23℃ | ISO 180 | 66 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.