Material Description
- Material Properties:Ozone resistant|Oil resistant
- Application Areas:pipeline|Automotive Applications
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| transmissivity | 3000μm | ASTM D1003 | 92.0 % |
| Refractive index | ASTM D542 | 1.531 | |
| Transmittance rate | ASTM D1003/ISO 13468 | 93 % |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 2500 Mpa | |
| tensile strength | ISO 527-2 | 71.0 Mpa | |
| Tensile strain | Break | ISO 527-2 | 10 % |
| Bending modulus | ISO 178 | 2500 Mpa | |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 21 kg·cm/cm(J/M)ft·lb/in | |
| Elongation at Break | ASTM D638/ISO 527 | 10 kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 2500 kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 104 kg/cm²(MPa)[Lb/in²] | |
| tensile strength | ASTM D638/ISO 527 | 71 kg/cm²(MPa)[Lb/in²] | |
| Tensile modulus | ASTM D638/ISO 527 | 2500 kg/cm²(MPa)[Lb/in²] |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Glass transition temperature | JISK7121 | 139 °C | |
| Linear coefficient of thermal expansion | MD | ASTME831 | 6E-05 cm/cm/°C |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 122 ℃(℉) |
| Combustibility (rate) | UL 94 | hb |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 280°C/2.16kg | JISK6719 | 25 g/10min |
| Water absorption rate | Equilibrium | ASTM D570 | <0.010 % |
| Shrinkage rate | ASTM D955 | 1.01 % | |
| melt mass-flow rate | ASTM D1238/ISO 1133 | 25 g/10min |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Volume resistivity | ASTM D257/IEC 60093 | 1.0E+16 Ω.cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.