Material Description
- Material Properties:High toughness|copolymer
- Application Areas:--
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ball-indentation hardness | H358/30 | ISO 2039-1 | 88.0 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火 | ISO 75-2/A | 75.0 °C |
melting temperature | ISO 11357-3 | 166 °C | |
Linear coefficient of thermal expansion | MD:23到55°C | ISO 11359-2 | 1.4E-04 cm/cm/°C |
maximum service temperature | 短周期操作 | 100 °C |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
ISOType | ISO 9988-1 | POM-K.M-GNPR.01-001 |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 8.5 kJ/m² |
23°C | ISO 179/1eA | 15 kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 240 kJ/m² |
23°C | ISO 179/1eU | 无断裂 |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.30 g/cm³ | |
Apparent density | 0.85 g/cm³ | ||
Melt volume flow rate | 190°C/2.16kg | ISO 1133 | 3.00 cm3/10min |
shrinkage rate | TD | ISO 294-4 | 1.8 % |
MD | ISO 294-4 | 1.8 % | |
Water absorption rate | 饱和,23°C | ISO 62 | 0.90 % |
平衡,23°C,50%RH | ISO 62 | 0.20 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC 60093 | 1E+15 ohms | |
volume resistivity | IEC 60093 | 1E+14 ohms·cm | |
relative permittivity | 1MHz | IEC 60250 | 3.40 |
Dissipation Factor | 1MHz | IEC 60250 | 8E-03 |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 0 |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 1700 Mpa | |
tensile strength | 屈服 | ISO 527-2/50 | 40.0 Mpa |
Tensile strain | 屈服 | ISO 527-2/50 | 7.3 % |
Nominal tensile fracture strain | ISO 527-2/50 | >50 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.