TPEE Hytrel® HTR8441 BK316 DUPONT USA
107
- Unit Price:US$ 8,500 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:50MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Dongguan Kenai New Material Co., Ltd.
+86 1324********View
kntp********View
For more details, please contact the supplier!
Material Description
- Material Properties:High temperature resistance|Chemical resistance
- Application Areas:Automotive Applications|Cable|Blow molding applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| Filling analysis | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| ThermalConductivityofMelt | 0.16 | W/m/K | ||
| SpecificHeatCapacity of Melt | 2150 | J/kg/°C | ||
| Melt density | 1.01 | g/cm³ | ||
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of cantilever beam gap | 23°C | ISO 8256/1 | 330 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 无断裂 | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Burning rate | 1.00mm | ISO 3795 | 42 | mm/min |
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
| tear strength | Flow | ISO 34-1 | 140 | kN/m |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | 5.0%Strain | ISO 527-2 | 7.80 | Mpa |
| Break | ISO 527-2 | 35.0 | Mpa | |
| Tensile modulus | ISO 527-2 | 190 | Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 380 | % | |
| Tensile strain | Break | ISO 527-2 | >300 | % |
| tensile strength | 50%Strain | ISO 527-2 | 19.0 | Mpa |
| 10%Strain | ISO 527-2 | 11.9 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357-3 | 211 | °C | |
| Brittle temperature | ISO 974 | -54.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD | ISO 294-4 | 2.2 | % |
| TD | ISO 294-4 | 2.1 | % | |
| Melt Volume Flow Rate (MVR) | 240°C/10.0kg | ISO 1133 | 10.0 | cm3/10min |
| melt mass-flow rate | 240°C/10.0kg | ISO 1133 | 10 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD,15Sec | ISO 868 | 52 | |
| ShoreD | ISO 868 | 58 | ||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| Odor | VDA270 | 3.50 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Other Prices
| Supplier | Unit Price |
|---|---|
| ASIAPLAS | US$ 6820 /MT |