Material Description
- Material Properties:High impact resistance|High temperature resistance|Flame retardant|Glass fiber reinforced|High mobility|enhance|Low temperature resistance|Filler: Glass fiber reinforced material|30%|Filler by weight
- Application Areas:Fiber grade
- Color:--
- Grade:Enhanced level
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 30 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.35mm | UL 94 | V-0 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Taber abraser | 1000Cycles | ISO 9352 | 45.0 | mg |
| bending strength | 23°C | ISO 178 | 220 | Mpa |
| Bending modulus | 23°C | ISO 178 | 12000 | Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 1.5 | % |
| tensile strength | Yield,23°C | ISO 527-2 | 140 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2.6E-05 | cm/cm/°C |
| Melting temperature | ISO 11357-3 | 278 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 260 | °C |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 3.9E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.020 | % |
| Shrinkage rate | MD:3.00mm4 | Internal Method | 0.30 | % |
| TD:3.00mm2 | Internal Method | 0.90 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 23°C,1MHz | IEC 60250 | 2E-03 | |
| Dielectric constant | 23°C,1MHz | IEC 60250 | 3.20 | |
| Dielectric strength | IEC 60243-1 | 23 | KV/mm | |
| Volume resistivity | IEC 60093 | 1E+16 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ISO 2039-2 | 120 | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| BarFlowLength | 320°C,1.00mm | Internal Method | 170 | mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.