Material Description
- Material Properties:high strength|Glass fiber reinforced|enhance|Flame retardant|High rigidity
- Application Areas:Casters|Electrical applications
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | 东丽法 | 0.20 % | |
东丽法 | 0.70 % | ||
东丽法 | 124 |
other | Test Condition | Test Method | Test Result |
---|---|---|---|
Color | 本色.黑 |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D-570 | 0.02 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 30 kg·cm/cm(J/M)ft·lb/in | |
tensile strength | ASTM D638/ISO 527 | 165 kg/cm²(MPa)[Lb/in²] | |
elongation | ASTM D638/ISO 527 | 1.4 % | |
Rockwell hardness | ASTM D785 | R-123 | |
bending strength | ASTM D790/ISO 178 | 250 kg/cm²(MPa)[Lb/in²] | |
limiting pv value | 东丽法 | 东丽法 KJ/m | |
bending strength | ASTM D-790 | 13.7 GPa | |
tensile strength | ASTM D-638 | 155 Mpa | |
ASTM D-638 | 1.6 % | ||
elongation at break | ASTM D-732 | 75 | |
Shore hardness | ASTM D-785 | 120 洛氏 | |
coefficient of friction | ASTM D-1894 | 0.25 | |
Impact strength of cantilever beam gap | ASTM D-256 | 100 J/m | |
ASTM D-256 | 30 KJ/m | ||
bending strength | ASTM D-790 | 205 Mpa | |
abrasion | ASTM D-1044 | 50 mg/1000回 |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
dielectric constant | ASTM D150/IEC 60250 | 3.6 | |
Volume resistivity | ASTM D257/IEC 60093 | 10^14 Ω.cm | |
dielectric constant | ASTM D-150 | 3.8 | |
arc resistance | ASTM D-495 | 127 秒 | |
dielectric strength | ASTM D-149 | 21 MV/m | |
Inherent resistance of volume | ASTM D-257 | 10 Ω.m | |
Induced positive connection | ASTM D-150 | 0.002 |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1660 | |
Water absorption rate | ASTM D570/ISO 62 | 0.02 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Combustibility (rate) | UL 94 | V-0 (0.28mmt) | |
Heat distortion temperature | ASTM D648/ISO 75 | >260 ℃(℉) | |
Linear coefficient of thermal expansion | ASTM D-696 | 2.2 | |
ASTM D-696 | 3.3 | ||
Heat distortion temperature | ASTM D-648 | >260 °C | |
combustibility | UL -94 | V-0 | |
melting temperature | DSC | 278 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.