PC/PET XYLEX™  X7300 SABIC INNOVATIVE US

506
  • Unit Price:US$ 4,110 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    72MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    Guangzhou port, China
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:UV resistanceHigh mobility
  • Application Areas:Automotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

optical performanceTest ConditionTest MethodTest ResultTest Unit
turbidity2540μmASTM D10032.0%
transmissivity2540μmASTM D100388.0%
impact performanceTest ConditionTest MethodTest ResultTest Unit
Dart impact23°C,TotalEnergyASTM D376395.0J
Impact strength of cantilever beam gap23°CISO 180/1A9.0kJ/m²
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile strainYieldISO 527-2/505.0%
elongationYieldASTM D6385.0%
tensile strengthBreakISO 527-2/5055.0Mpa
tensile strengthBreakASTM D63852.0Mpa
tensile strengthYieldISO 527-2/5055.0Mpa
tensile strengthYieldASTM D63849.0Mpa
Tensile modulusISO 527-2/11900Mpa
Tensile modulusASTM D6381840Mpa
elongationBreakASTM D638150%
Tensile strainBreakISO 527-2/50>150%
Bending modulus50.0mmSpanASTM D7901940Mpa
Bending modulusISO 1782000Mpa
bending strengthISO 17871.0Mpa
bending strengthYield,50.0mmSpanASTM D79083.0Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionMD:23to60°CISO 11359-28.5E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8311.2E-04cm/cm/°C
Vicat softening temperatureISO 306/B120106°C
Vicat softening temperatureASTM D15259108°C
Hot deformation temperature1.8MPa,Unannealed,100mmSpanISO 75-2/Ae90.0°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64888.0°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648102°C
Linear coefficient of thermal expansionTD:23to60°CISO 11359-28.5E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8311.1E-04cm/cm/°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateTD:3.20mmInternal Method0.50-0.70%
Shrinkage rateMD:3.20mmInternal Method0.40-0.80%
Melt Volume Flow Rate (MVR)265°C/2.16kgISO 113321.0cm3/10min
melt mass-flow rate265°C/2.16kgASTM D123821g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China