Material Description
- Material Properties:Flame retardant
- Application Areas:Spool|Shell|switch|Home appliance components|Electronic field|Electrical field
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | -30°C | ASTM D256 | 22 | J/m |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak | |
| -30°C | ISO 179/1eU | NoBreak | ||
| Charpy Notched Impact Strength | 23°C | ISO 179/2C | 4.0 | kJ/m² |
| 23°C10 | ISO 179/1eA | 8.0 | kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 37 | J/m |
| -30°C | ISO 180/1A | 3.0 | kJ/m² | |
| 23°C | ISO 180/1A | 5.0 | kJ/m² | |
| Charpy Notched Impact Strength | -30°C10 | ISO 179/1eA | 4.0 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ASTM D4812 | 1600 | J/m |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | NoBreak | |
| 23°C | ISO 180/1U | NoBreak | ||
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 200 | J |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.71mm | UL 94 | V-0 | |
| 3.0mm | UL 94 | 5VA | ||
| Burning wire flammability index | 1.0mm | IEC 60695-2-12 | 960 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 30 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2/1 | 2800 | Mpa | |
| ASTM D638 | 2820 | Mpa | ||
| tensile strength | Break | ISO 527-2/50 | 40.0 | Mpa |
| Break | ASTM D638 | 58.0 | Mpa | |
| Yield | ISO 527-2/50 | 55.0 | Mpa | |
| Yield | ASTM D638 | 58.0 | Mpa | |
| Tensile strain | Yield | ASTM D638 | 20 | % |
| Yield | ISO 527-2/50 | 6.0 | % | |
| elongation | Break | ASTM D638 | 20 | % |
| Tensile strain | Break | ISO 527-2/50 | 20 | % |
| Bending modulus | 50.0mmSpan | ASTM D790 | 2620 | Mpa |
| ISO 178 | 2600 | Mpa | ||
| bending strength | ISO 178 | 90.0 | Mpa | |
| Yield,50.0mmSpan | ASTM D790 | 101 | Mpa | |
| Taber abraser | 1000Cycles,1000g,CS-17Wheel | Internal Method | 19.0 | mg |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | -- | ISO 306/A50 | 212 | °C |
| Hot deformation temperature | 1.8MPa,Unannealed,100mmSpan12 | ISO 75-2/Ae | 60.0 | °C |
| 1.8MPa,Unannealed,64.0mmSpan13 | ISO 75-2/Af | 71.0 | °C | |
| Vicat softening temperature | ASTM D152514 | 165 | °C | |
| Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTM D648 | 162 | °C |
| Vicat softening temperature | -- | ISO 306/B50 | 165 | °C |
| -- | ISO 306/B120 | 165 | °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.9E-05 | cm/cm/°C |
| MD:60to138°C | ASTME831 | 1.3E-04 | cm/cm/°C | |
| MD:-40to40°C | ISO 11359-2 | 7.6E-05 | cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 135 | °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 74.0 | °C | |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 71.0 | °C | |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 1E-04 | cm/cm/°C |
| TD:-40to40°C | ASTME831 | 7.9E-05 | cm/cm/°C | |
| RTI Elec | UL 746 | 120 | °C | |
| RTI Imp | UL 746 | 120 | °C | |
| RTI Str | UL 746 | 140 | °C | |
| Linear coefficient of thermal expansion | TD:-40to40°C | ISO 11359-2 | 7.3E-05 | cm/cm/°C |
| TD:23to60°C | ISO 11359-2 | 1E-04 | cm/cm/°C | |
| thermal conductivity | ISO 8302 | 0.24 | W/m/K | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.080 | % |
| Saturation,23°C | ISO 62 | 0.36 | % | |
| Shrinkage rate | TD:--3 | Internal Method | 1.6-2.4 | % |
| TD:--4 | Internal Method | 1.0-1.7 | % | |
| TD:--2 | Internal Method | 0.90-1.9 | % | |
| MD:3.20mm | Internal Method | 1.5-2.3 | % | |
| MD:--4 | Internal Method | 0.90-1.6 | % | |
| MD:--3 | Internal Method | 1.5-2.3 | % | |
| MD:--2 | Internal Method | 1.1-1.8 | % | |
| Melt Volume Flow Rate (MVR) | 250°C/2.16kg | ISO 1133 | 8.00 | cm3/10min |
| melt mass-flow rate | 250°C/2.16kg | ASTM D1238 | 8.6 | g/10min |
| density | ISO 1183 | 1.40 | g/cm³ | |
| Specific volume | ASTM D792 | 0.710 | cm³/g | |
| density | ASTM D792 | 1.40 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 1.60mm,in Oil | ASTM D149 | 22 | KV/mm |
| 3.20mm,inAir | ASTM D149 | 18 | KV/mm | |
| 0.800mm,in Oil | IEC 60243-1 | 31 | KV/mm | |
| 1.00mm15 | IEC 60243-1 | 18 | KV/mm | |
| Relative permittivity | 1MHz | IEC 60250 | 2.80 | |
| Dielectric strength | 1.60mm,in Oil | IEC 60243-1 | 24 | KV/mm |
| 3.20mm,in Oil | IEC 60243-1 | 15 | KV/mm | |
| Relative permittivity | 50Hz | IEC 60250 | 2.90 | |
| 60Hz | IEC 60250 | 2.90 | ||
| 100Hz | IEC 60250 | 3.10 | ||
| Dissipation factor | 50Hz | IEC 60250 | 1E-03 | |
| 60Hz | IEC 60250 | 1E-03 | ||
| 100Hz | IEC 60250 | 2E-03 | ||
| 1MHz | IEC 60250 | 0.010 | ||
| Arc resistance | ASTM D495 | PLC6 | ||
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 3 | |
| -- | IEC 60112 | PLC 3 | ||
| SolutionB | IEC 60112 | PLC 4 | ||
| High arc combustion index | HAI | UL 746 | PLC 0 | |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 4 | |
| Surface resistivity | IEC 60093 | >1.0E+15 | ohms | |
| Volume resistivity | IEC 60093 | >1.0E+15 | ohms·cm | |
| Hot wire ignition | HWI | UL 746 | PLC 2 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ISO 2039-2 | 120 | |
| Ball Pressure Test | H358/30 | ISO 2039-1 | 105 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.