ASA/PC GELOY™ XTPMFR10 BK1E397L SABIC INNOVATIVE SHANGHAI
8
- Unit Price:US$ 3,900 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:15MT
- Delivery Terms:FOB
- Port of Loading :Shanghai port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Huizhou Rijing Chemical Technology Co., Ltd.
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Thermal stability|Antistatic|High mobility
- Application Areas:Automotive Applications|Electrical applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| Filling analysis | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Melt viscosity | 260°C, 1500 sec^-1 | ISO 11443 | 105 | Pa·s |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Multi axis Instrumented Impact Energy | ISO 6603-2 | 85.0 | J | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.0 mm | UL 94 | V-0 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | --2 | ASTM D638 | 2680 | Mpa |
| -- | ISO 527-2/1 | 2680 | Mpa | |
| tensile strength | Yield3 | ASTM D638 | 65.0 | Mpa |
| Yield4 | ASTM D638 | 60.0 | Mpa | |
| Yield | ISO 527-2/5 | 61.0 | Mpa | |
| Yield | ISO 527-2/50 | 66.0 | Mpa | |
| bending strength | ISO 178 | 97.0 | Mpa | |
| Bending modulus | ISO 178 | 2720 | Mpa | |
| elongation | Break | ISO 527-2/50 | 21 | % |
| Break | ISO 527-2/5 | 50 | % | |
| Break3 | ASTM D638 | 31 | % | |
| Break4 | ASTM D638 | 58 | % | |
| Yield | ISO 527-2/5 | 4.0 | % | |
| Yield3 | ASTM D638 | 4.0 | % | |
| Yield4 | ASTM D638 | 4.0 | % | |
| tensile strength | Break | ISO 527-2/50 | 47.0 | Mpa |
| Break | ISO 527-2/5 | 46.0 | Mpa | |
| Break3 | ASTM D638 | 47.0 | Mpa | |
| Break4 | ASTM D638 | 49.0 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Suggested maximum moisture content | 0.020 | % | ||
| Hopper temperature | 60 to 80 | °C | ||
| drying time | 2.0 to 4.0 | hr | ||
| drying temperature | 80 to 90 | °C | ||
| Temperature at the rear of the barrel | 200 to 230 | °C | ||
| Temperature in the middle of the barrel | 220 to 260 | °C | ||
| Temperature at the front of the material cylinder | 230 to 270 | °C | ||
| Spray nozzle temperature | 220 to 260 | °C | ||
| Processing (melt) temperature | 230 to 270 | °C | ||
| Mold temperature | 50 to 70 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | Across Flow : -40°C | ISO 11359-2 | 6.3E-5 | cm/cm/°C |
| Flow : -40 to 40°C | ISO 11359-2 | 6.3E-5 | cm/cm/°C | |
| Vicat softening temperature | -- | ISO 306/B120 | 98.0 | °C |
| -- | ISO 306/B50 | 96.0 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm, 64.0 mm Span | ISO 75-2/Af | 81.0 | °C |
| 0.45 MPa, Unannealed, 4.00 mm, 64.0 mm Span | ISO 75-2/Bf | 90.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | 260°C/2.16 kg | ISO 1133 | 30.0 | cm3/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.