PC MOCREATE® DCM01-3101 NINGBO ZHETIE DAFENG
275
- Unit Price:US$ 2,545 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High temperature resistance|Easy electroplating|Flame retardant
- Application Areas:Automotive sector|Electronic field|Electrical field
- Color:--
- Grade:Halogen-free flame retardant grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23℃,3.2mm | ASTM D256 | 75 J/m |
| 23℃,4.0mm | ISO 180 | 8 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Bending modulus | 2mm/min | ISO 178 | 3600 Mpa |
| bending strength | 2mm/min | ISO 178 | 110 Mpa |
| Tensile strain | Break,50mm/min | ISO 527-1 | 3.5 % |
| tensile strength | 50mm/min | ISO 527-1 | 82 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa | ISO 75-1 | 135 °C |
| 0.45MPa | ISO 75-1 | 140 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| ash content | ISO 3154.1 | 9-10 % | |
| Water absorption rate | ISO 960 | ≤0.3 % | |
| Shrinkage rate | 2mm flow | ISO 294-4 | 0.2-0.4 % |
| melt mass-flow rate | 300℃,1.2kg | ISO 1133 | 9 g/10min |
| density | 23℃/H2O | ISO 1183-1 | 1.25 g/cm³ |
| flame retardant performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 1.6 mm | UL 94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.