ABS Toyolac®  100-322 TORAY JAPAN

80
  • Unit Price:US$ 1,984 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High impact
  • Application Areas:Automotive sectorElectronic and electrical fieldElectrical appliances
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°C,12.7mmASTM D256230J/m
Impact strength of cantilever beam gap23°C,3.20mmASTM D256270J/m
Impact strength of cantilever beam gap0°C,12.7mmASTM D256180J/m
Impact strength of cantilever beam gap0°C,3.20mmASTM D256200J/m
Impact strength of cantilever beam gap-30°C,12.7mmASTM D256120J/m
Impact strength of cantilever beam gap-30°C,3.20mmASTM D256140J/m
Charpy Notched Impact Strength23°CISO 179/1eA20kJ/m²
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant ratingUL 94HB
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
crackISO 527-2/50>10%
crackASTM D63848%
yieldISO 527-2/5051.0Mpa
yieldASTM D63848.0Mpa
Tensile modulusISO 527-2/12600Mpa
--5ISO 17878.0Mpa
--4ASTM D79074.0Mpa
Bending modulusASTM D7902280Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionMDASTM D6967.4E-05cm/cm/°C
thermal conductivityASTMC1770.15W/m/K
1.8MPa, unannealedISO 75-2/A83.0°C
1.8MPa, unannealed, 12.7mmASTM D64893.0°C
1.8MPa, unannealed, 6.40mmASTM D64888.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rate23°C,24hrASTM D5700.30%
Shrinkage rateMDASTM D9550.40-0.60%
melt mass-flow rate220°C/10.0kgISO 113315g/10min
densityASTMD7921.04g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Surface resistivityASTM D257>1.0E+16ohms
Volume resistivity23°CASTM D257>1.0E+16ohms·cm
Dielectric strengthASTM D14923KV/mm
Dielectric constant1kHzASTM D1503.10
Dissipation factor1kHzASTM D1506.6E-03
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardnessR-ScaleASTM D785112
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China