PC/ABS LNP™ FARADEX™  NS0031 SABIC INNOVATIVE US

203
  • Unit Price:US$ 8,533 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    33MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    Guangzhou port, China
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High mobilityFlame retardant
  • Application Areas:CastersElectrical applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°CISO 180/1A9.5kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U32kJ/m²
Dart impact23°C,EnergyatPeakLoadASTM D376315.0J
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile modulusASTM D6383110Mpa
Tensile modulusISO 527-2/12700Mpa
tensile strengthYieldASTM D63852.4Mpa
tensile strengthYieldISO 527-250.0Mpa
tensile strengthBreakASTM D63849.6Mpa
tensile strengthBreakISO 527-246.0Mpa
elongationYieldASTM D6383.3%
Tensile strainYieldISO 527-23.5%
elongationBreakASTM D6384.7%
Tensile strainBreakISO 527-26.0%
Bending modulusASTM D7902990Mpa
Bending modulusISO 1782800Mpa
bending strengthASTM D79089.6Mpa
bending strengthISO 17886.0Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpanISO 75-2/Bf115°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D648105°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO 75-2/Af103°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8317.7E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO 11359-25.9E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8316.3E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO 11359-28.2E-05cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648120°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateMD:24hrASTM D9550.30%
Shrinkage rateTD:24hrASTM D9550.35%
Shrinkage rateTD:24hrISO 294-40.35%
Shrinkage rateMD:24hrISO 294-40.30%
Water absorption rate24hr,50%RHASTM D5700.10%
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Surface resistivityASTM D25710to1.0E+3ohms
Volume resistivityASTM D2571E+04ohms·cm
Shielding effectiveness (EMI)3.00mmInternal Method50to65dB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.