PC/PBT XENOY™ 5720U-1001 SABIC INNOVATIVE US
20
- Unit Price:US$ 3,070 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Dongguan Saigeli Plasticization Co., Ltd
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Chemical resistance|Low temperature impact resistance
- Application Areas:Plastic bag|Lighting applications|Household daily necessities
- Color:--
- Grade:Cold resistant grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 47 | kJ/m² |
| 23°C | ISO 179/1eA | 55 | kJ/m² | |
| Dart impact | -40°C, Energy at Peak | ASTM D3763 | 49.0 | J |
| -40°C, Total Energy | ASTM D3763 | 59.0 | J | |
| -30°C, Energy at Peak | ASTM D3763 | 49.0 | J | |
| -30°C, Total Energy | ASTM D3763 | 61.0 | J | |
| -20°C, Energy at Peak | ASTM D3763 | 41.0 | J | |
| -20°C, Total Energy | ASTM D3763 | 53.0 | J | |
| 23°C, Energy at Peak | ASTM D3763 | 44.0 | J | |
| 23°C, Total Energy | ASTM D3763 | 54.0 | J | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | --2 | ASTM D638 | 1830 | Mpa |
| --3 | Internal Method | 1830 | Mpa | |
| --4 | ASTM D638 | 1810 | Mpa | |
| -- | ISO 527-2/1 | 1790 | Mpa | |
| tensile strength | Yield5 | ASTM D638 | 47.0 | Mpa |
| Yield6 | Internal Method | 45.0 | Mpa | |
| Yield7 | ASTM D638 | 44.0 | Mpa | |
| Yield | ISO 527-2/5 | 44.0 | Mpa | |
| Yield | ISO 527-2/50 | 47.0 | Mpa | |
| Break7 | ASTM D638 | 50.0 | Mpa | |
| Break6 | Internal Method | 47.0 | Mpa | |
| Break5 | ASTM D638 | 48.0 | Mpa | |
| Break | ISO 527-2/5 | 43.0 | Mpa | |
| elongation | Yield7 | ASTM D638 | 4.6 | % |
| Yield6 | Internal Method | 4.6 | % | |
| Yield5 | ASTM D638 | 4.0 | % | |
| Yield | ISO 527-2/5 | 4.1 | % | |
| Yield | ISO 527-2/50 | 4.6 | % | |
| Break7 | ASTM D638 | 120 | % | |
| Break6 | Internal Method | 110 | % | |
| Break5 | ASTM D638 | 120 | % | |
| Break | ISO 527-2/5 | 110 | % | |
| Break | ISO 527-2/50 | 120 | % | |
| Bending modulus | 50.0 mm Span8 | ASTM D790 | 1660 | Mpa |
| --9 | ISO 178 | 1860 | Mpa | |
| bending strength | --9,10 | ISO 178 | 71.0 | Mpa |
| Yield, 50.0 mm Span8 | ASTM D790 | 70.0 | Mpa | |
| Break, 50.0 mm Span8 | ASTM D790 | 69.0 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Exhaust hole depth | 0.013 to 0.020 | mm | ||
| Screw speed | 50 to 80 | rpm | ||
| Back pressure | 0.300 to 0.700 | Mpa | ||
| Mold temperature | 65 to 90 | °C | ||
| Processing (melt) temperature | 260 to 275 | °C | ||
| Spray nozzle temperature | 255 to 270 | °C | ||
| Temperature at the front of the material cylinder | 255 to 275 | °C | ||
| Temperature in the middle of the barrel | 250 to 270 | °C | ||
| Temperature at the rear of the barrel | 245 to 265 | °C | ||
| Suggested injection volume | 50 to 80 | % | ||
| Suggested maximum moisture content | 0.020 | % | ||
| drying time | 4.0 to 6.0 | hr | ||
| drying temperature | 110 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45 MPa, Unannealed, 3.20 mm | ASTM D648 | 108 | °C |
| Linear coefficient of thermal expansion | Across Flow : -30 to 80°C | ISO 11359-2 | 1.0E-4 | cm/cm/°C |
| Across Flow : -40 to 95°C | ASTM E831 | 1.0E-4 | cm/cm/°C | |
| Flow : -30 to 80°C | ISO 11359-2 | 9.8E-5 | cm/cm/°C | |
| Flow : -40 to 95°C | ASTM E831 | 9.8E-5 | cm/cm/°C | |
| Vicat softening temperature | -- | ISO 306/B120 | 122 | °C |
| -- | ASTM D152513 | 119 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm, 64.0 mm Span12 | ISO 75-2/Af | 87.0 | °C |
| 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 95.0 | °C | |
| 1.8 MPa, Unannealed, 3.20 mm | ASTM D648 | 83.0 | °C | |
| 0.45 MPa, Unannealed, 4.00 mm, 64.0 mm Span12 | ISO 75-2/Bf | 109 | °C | |
| 0.45 MPa, Unannealed, 6.40 mm | ASTM D648 | 117 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Specific volume | ASTM D792 | 0.850 | cm³/g | |
| melt mass-flow rate | 250°C/2.16 kg | ASTM D1238 | 3.8 | g/10 min |
| 250°C/5.0 kg | ASTM D1238 | 11 | g/10 min | |
| 265°C/2.16 kg | ASTM D1238 | 6.0 | g/10 min | |
| 266°C/5.0 kg | ASTM D1238 | 20 | g/10 min | |
| 250°C/2.16 kg | ISO 1133 | 3.0 | g/10 min | |
| Melt Volume Flow Rate (MVR) | 250°C/2.16 kg | ISO 1133 | 3.00 | cm3/10min |
| 250°C/5.0 kg | ISO 1133 | 10.0 | cm3/10min | |
| 265°C/2.16 kg | ISO 1133 | 6.00 | cm3/10min | |
| 265°C/5.0 kg | ISO 1133 | 18.0 | cm3/10min | |
| Shrinkage rate | 3.20 mm,Flow | Internal Method | 1.0 - 1.2 | % |
| Water absorption rate | Saturation, 23°C | ISO 62 | 0.28 | % |
| Equilibrium, 23°C, 50% RH | ISO 62 | 0.080 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.