PEEK VICTREX® 450GL20 VICTREX UK
300
- Unit Price:US$ 85,577 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:50MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:high strength|Glass fiber reinforced
- Application Areas:Non specific food|Medical supplies|Nursing supplies
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.43 g/cm³ | |
spiral flow length | 内部方法 | 10.0 CM | |
Shrinkage rate | ISO 294-4 | 0.90 % | |
ISO 294-4 | 0.30 % | ||
Water absorption rate | ISO 62 | 0.40 % | |
ISO 62 | 0.45 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ISO 868 | 86 |
Filling analysis | Test Condition | Test Method | Test Result |
---|---|---|---|
melt viscosity | ISO 11443 | 475 Pa·s |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Flexural modulus | ISO 178 | 8300 Mpa | |
bending strength | ISO 178 | 250 Mpa | |
Tensile modulus | ISO 527-2 | 8800 Mpa | |
tensile strength | ISO 527-2 | 160 Mpa | |
Tensile strain | ISO 527-2 | 3.4 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180/A | 10 kJ/m² | |
Suspended wall beam without notch impact strength | ISO 180 | 65 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+16 ohms·cm | |
dielectric strength | IEC 60243-1 | 24 KV/mm | |
dielectric constant | IEC 60250 | 3.10 | |
Dissipation Factor | IEC 60250 | 5E-03 | |
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | V |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | ISO 11359-2 | 4.5E-05 cm/cm/°C | |
ISO 11359-2 | 1.2E-04 cm/cm/°C | ||
thermal conductivity | ISO 22007-4 | 0.30 W/m/K | |
ISO 22007-4 | 0.35 W/m/K | ||
Heat distortion temperature | ISO 75-2/Af | 315 °C | |
Glass Transition Temperature | ISO 11357-2 | 143 °C | |
ISO 11357-2 | 150 °C | ||
melting temperature | ISO 11357-3 | 343 °C | |
Linear coefficient of thermal expansion | ISO 11359-2 | 2E-05 cm/cm/°C | |
ISO 11359-2 | 2.2E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.