PPO NORYL™ 731S-701S SABIC INNOVATIVE SHANGHAI
325
- Unit Price:US$ 4,845 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:48MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility|Antistatic|High temperature resistance|currency
- Application Areas:Food containers
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt volume flow rate | ISO 1133 | 8.00 cm3/10min | |
Water absorption rate | ISO 62 | 0.23 % | |
ISO 62 | 0.060 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 2300 Mpa | |
tensile strength | ISO 527-2/50 | 55.0 Mpa | |
ISO 527-2/50 | 50.0 Mpa | ||
Tensile strain | ISO 527-2/50 | 5.0 % | |
ISO 527-2/50 | 30 % | ||
Flexural modulus | ISO 178 | 2200 Mpa | |
bending strength | ISO 178 | 75.0 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 5.0 kJ/m² | |
ISO 179/1eA | 15 kJ/m² | ||
Impact strength of cantilever beam gap | ISO 180/1A | 5.0 kJ/m² | |
ISO 180/1A | 15 kJ/m² |
injection | Test Condition | Test Method | Test Result |
---|---|---|---|
drying temperature | 100 to 120 °C | ||
drying time | 2.0 to 3.0 hr | ||
Hopper temperature | 60 to 80 °C | ||
Temperature at the rear of the barrel | 240 to 260 °C | ||
Temperature in the middle of the barrel | 260 to 280 °C | ||
Temperature at the front of the material cylinder | 280 to 300 °C | ||
Spray nozzle temperature | 260 to 280 °C | ||
Processing (melt) temperature | 280 to 300 °C | ||
Temperature | 80 to 120 °C |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/Ae | 115 °C | |
vicat | ISO 306/B50 | 135 °C | |
ISO 306/B120 | 140 °C | ||
Linear coefficient of thermal expansion | ISO 11359-2 | 7.0E-5 cm/cm/°C | |
ISO 11359-2 | 7.0E-5 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.