PA46 Stanyl® TW241F8 NC DSM HOLAND
182
- Unit Price:US$ 6,134 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:86.1MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Lubricity|Thermal stability
- Application Areas:Automotive Applications|Home appliance components
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.51 g/cm³ | |
Shrinkage rate | ISO 294-4 | 1.1 % | |
ISO 294-4 | 0.50 % | ||
Water absorption rate | ISO 62 | 2.2 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flammability level | UL 94 | HB | |
UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 13000 Mpa | |
ISO 527-2 | 6900 Mpa | ||
ISO 527-2 | 6100 Mpa | ||
ISO 527-2 | 5700 Mpa | ||
ISO 527-2 | 5300 Mpa | ||
tensile strength | ISO 527-2 | 230 Mpa | |
ISO 527-2 | 130 Mpa | ||
ISO 527-2 | 115 Mpa | ||
ISO 527-2 | 105 Mpa | ||
ISO 527-2 | 100 Mpa | ||
Tensile strain | ISO 527-2 | 3.0 % | |
ISO 527-2 | 6.5 % | ||
ISO 527-2 | 6.5 % | ||
ISO 527-2 | 6.5 % | ||
ISO 527-2 | 6.5 % | ||
Flexural modulus | ISO 178 | 11500 Mpa | |
ISO 178 | 5800 Mpa | ||
ISO 178 | 5200 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 12 kJ/m² | |
ISO 179/1eA | 14 kJ/m² | ||
Impact strength of simply supported beam without notch | ISO 179/1eU | 75 kJ/m² | |
ISO 179/1eU | 95 kJ/m² | ||
Impact strength of cantilever beam gap | ISO 180/1A | 12 kJ/m² | |
ISO 180/1A | 14 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 1.0E+14 ohms·cm | |
dielectric strength | IEC 60243-1 | 30 KV/mm | |
relative permittivity | IEC 60250 | 4.30 | |
IEC 60250 | 4.00 | ||
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 2 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/B | 290 °C | |
ISO 75-2/A | 290 °C | ||
melting temperature | ISO 11357-3 | 295 °C | |
Linear coefficient of thermal expansion | ISO 11359-2 | 2.5E-5 cm/cm/°C | |
ISO 11359-2 | 5.0E-5 cm/cm/°C | ||
RTI Elec | UL 746 | 65.0 °C | |
Thermal Index - 5000 hr | IEC 60216 | 177 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.