plas

PA66 LNP™ LUBRICOMP™  RN001 BK1B599 SABIC INNOVATIVE US

236
  • Unit Price:US$ 6,288 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    61MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Thermal stabilityUV resistance
  • Application Areas:Electrical applicationsHome appliance components
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 180/1A2.8 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U54 kJ/m²
Dart impact23°C,EnergyatPeakLoadASTM D37632.30 J
mechanical propertiesTest ConditionTest MethodTest Result
Friction coefficientStaticASTM D3702Modified0.55
Wear factorWasherASTM D3702Modified103 10^-10in^5-min/ft-lb-hr
tensile strengthBreakASTM D63884.1 Mpa
tensile strengthBreakISO 527-269.0 Mpa
elongationYieldASTM D6382.9 %
Tensile strainYieldISO 527-22.1 %
elongationBreakASTM D6383.8 %
Tensile strainBreakISO 527-242 %
Bending modulusASTM D7903450 Mpa
Bending modulusISO 1783400 Mpa
bending strengthISO 178107 Mpa
Friction coefficientDynamicASTM D3702Modified0.75
Tensile modulusASTM D6384140 Mpa
Tensile modulusISO 527-2/13910 Mpa
tensile strengthYieldASTM D63884.1 Mpa
tensile strengthYieldISO 527-269.0 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO 75-2/Af301 °C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTM D648231 °C
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpanISO 75-2/Bf223 °C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64876.7 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateTD:24hrISO 294-41.0 %
Shrinkage rateMD:24hrISO 294-41.0 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.