Material Description
- Material Properties:Photostability|High impact resistance
- Application Areas:Electronic and electrical components|Pneumatic applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | -- Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Melting temperature | ISO 11357-3 | 130 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.05 g/cm³ | |
Melt Volume Flow Rate (MVR) | 275℃,5 kg275℃/5.0 kg | ISO 1133 | 180 cm3/10min |
Water absorption rate | Saturation,23℃Saturation, 73°F | ISO 62 | 5 % |
Equilibrium,23℃,50% RHEquilibrium, 73°F, 50% RH | ISO 62 | 2 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | MD,YieldMD : Yield | ISO 527-3 | 30 Mpa |
TD,YieldTD : Yield | ISO 527-3 | 28 Mpa | |
MD,BreakMD : Break | ISO 527-3 | 85 Mpa | |
TD,BreakTD : Break | ISO 527-3 | 55 Mpa | |
Tensile strain | MD,YieldMD : Yield | ISO 527-3 | 15 % |
TD,YieldTD : Yield | ISO 527-3 | 8 % | |
MD,BreakMD : Break | ISO 527-3 | 800 % | |
TD,BreakTD : Break | ISO 527-3 | 900 % | |
Elmendorf tear strength | MDMD | ISO 6383-2 | 80 N |
TDTD | ISO 6383-2 | 80 N | |
Tear resistance of pants type | MDMD | ISO 6383-1 | 65 N/mm |
TDTD | ISO 6383-1 | 65 N/mm | |
Water vapor permeability | 23℃,85% RH23℃,85% RH | DIS 15106-1/-2 | 15 g/m²/24 hr |
Oxygen permeability | 23℃23°C 22 | DIS 15105-1/-2 | 120 cm³/m²/bar/24 hr |
23℃23°C 33 | DIS 15105-1/-2 | 200 cm³/m²/bar/24 hr | |
Carbon dioxide transmittance | 23℃23°C 22 | DIS 15105-1/-2 | 400 cm³/m²/bar/24 hr |
23℃23°C 33 | DIS 15105-1/-2 | 800 cm³/m²/bar/24 hr |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.