PA66 Zytel® BM70G20HSLX BK537 DUPONT USA
169
- Unit Price:US$ 3,080 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:52.3MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|enhance
- Application Areas:Automotive components|Electronic and Electrical Applications
- Color:--
- Grade:--
Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ball-indentation hardness | H961/30 | ISO 2039-1 | 225 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火 | ISO 75-2/B | 257 °C |
1.8MPa,未退火 | ISO 75-2/A | 239 °C | |
Glass Transition Temperature | ISO 11357-2 | 60.0 °C | |
melting temperature | ISO 11357-3 | 260 °C |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
FMVSS flammability | FMVSS302 | SE |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 40 kJ/m² |
23°C | ISO 179/1eU | 80 kJ/m² | |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 73 kJ/m² |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
MediumDensity | 1.07 g/cm³ | ||
MeltViscosity | 280°C,1000sec^-1 | ISO 11443 | 330000 mPa·s |
Ejection Temperature | 210 °C | ||
SpecificHeatCapacity of Melt | 2000 J/kg/°C | ||
ThermalConductivityofMelt | 0.20 W/m/K | ||
shrinkage rate | TD | ISO 294-4 | 0.70 % |
MD | ISO 294-4 | 0.50 % | |
Water absorption rate | 饱和,23°C,2.00mm | ISO 62 | 5.2 % |
平衡,23°C,2.00mm,50%RH | ISO 62 | 1.6 % | |
viscosity number | 96%H2SO4 | ISO 307 | 155 cm³/g |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile creep modulus | 1000hr | ISO 899-1 | -- Mpa |
flexural modulus | ISO 178 | 6000 Mpa | |
bending strength | ISO 178 | 160 Mpa | |
shear modulus | ISO 6721 | 1400 Mpa | |
Poisson's ratio | ISO 527 | -- | |
Tensile modulus | ISO 527-2 | 6500 Mpa | |
tensile strength | 断裂 | ISO 527-2 | 120 Mpa |
Tensile strain | 断裂 | ISO 527-2 | 4.0 % |
Tensile creep modulus | 1hr | ISO 899-1 | -- Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.