PP TIRIPRO® K8050 FCFC TAIWAN
484
- Unit Price:US$ 1,338 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20.9MT
- Delivery Terms:FOB
- Port of Loading :Kaoshiung port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility|High rigidity|High impact resistance|Excellent impact resistance|High liquidity|High rigidity
- Application Areas:Industrial applications|Automotive sector|Automotive supplies|Industrial components
- Color:--
- Grade:Impact resistant grade
Material Certification

TDS
Processing



SVHC
PSC

Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| FDA Compliance | 21 CFR Pt 177.1520 | Yes | ||
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230℃×2.16Kg | ASTM D-1238 | 50.0 | g/10min |
| Shrinkage rate | 23℃ | FCFC Method | 1.4-1.8 | % |
| density | 23℃/23℃ | ASTM D-792 | 0.90 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | 23℃,Yield | ASTM D-638 | 240 | kg/cm2 |
| Elongation at Break | 23℃ | ASTM D-638 | >200 | % |
| Bending modulus | 23℃ | ASTM D-790A | 12500 | kg/cm2 |
| Rockwell hardness | 23℃ | ASTM D-785 | 85 | R-Scale |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 10.0 | kg-cm/cm2 |
| -20℃ | ASTM D-256 | 5.0 | kg-cm/cm2 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | 1/16"HB | All Color | |
| Hot deformation temperature | 4.6kg/cm2 | ASTM D-648 | 115 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.