ASA GELOY™  XTWE270M-BR2B079 SABIC INNOVATIVE US

402
  • Unit Price:US$ 3,290 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    31MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    Guangzhou port, China
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Thermal stabilityAntistaticHigh mobility
  • Application Areas:Automotive ApplicationsElectrical applications
  • Color:--
  • Grade:--

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Dart impact23°C,TotalEnergyASTM D376328.0J
Impact strength of cantilever beam gap23°CISO 180/1A13kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A7.0kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA13kJ/m²
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
bending strengthYield,50.0mmSpanASTM D79056.0Mpa
bending strengthISO 17856.0Mpa
Bending modulus50.0mmSpanASTM D7901830Mpa
Tensile strainBreakISO 527-2/5028%
elongationBreakASTM D63838%
Tensile strainYieldISO 527-2/503.4%
elongationYieldASTM D6383.4%
tensile strengthBreakISO 527-2/5026.0Mpa
tensile strengthBreakASTM D63832.0Mpa
tensile strengthYieldISO 527-2/5036.0Mpa
tensile strengthYieldASTM D63836.0Mpa
Tensile modulusISO 527-2/11790Mpa
Tensile modulusASTM D6381910Mpa
Bending modulusISO 1781870Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Vicat softening temperature--ISO 306/B5082.0°C
Vicat softening temperatureASTM D15251085.0°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64869.0°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO 75-2/Af71.0°C
Vicat softening temperature--ISO 306/B12085.0°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8319.2E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO 11359-21E-04cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8311.1E-04cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO 11359-21.2E-04cm/cm/°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rateEquilibrium,23°C,50%RHISO 620.20%
Water absorption rateSaturation,23°CISO 620.80%
Shrinkage rateMD:3.20mmInternal Method0.30-0.70%
Melt Volume Flow Rate (MVR)220°C/5.0kgISO 11332.00cm3/10min
melt mass-flow rate220°C/10.0kgASTM D12389.7g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Other Prices

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China