Material Description
- Material Properties:Glass fiber reinforced|lubrication|Filler: Glass fiber reinforced material
- Application Areas:Electrical and Electronic Applications|Automotive components
- Color:--
- Grade:--
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| 23°C | ISO 180/1U | 26 | kJ/m² | |
| ASTM D4812 | 330 | J/m | ||
| ISO 180/1A | 7.8 | kJ/m² | ||
| ASTM D256 | 67 | J/m | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Wear factor | Washer | ASTM D3702Modified | 15.6 | 10^-10in^5-min/ft-lb-hr |
| Friction coefficient | Itself - Dynamic | ASTM D3702Modified | 0.52 | |
| bending strength | Break,50.0mmSpan | ASTM D790 | 201 | Mpa |
| Yield,50.0mmSpan | ASTM D790 | 202 | Mpa | |
| --5 | ISO 178 | 7220 | Mpa | |
| 50.0mm span | ASTM D790 | 6420 | Mpa | |
| crack | ISO 527-2/5 | 1.2 | % | |
| ASTM D638 | 3.0 | % | ||
| ISO 527-2/5 | 156 | Mpa | ||
| ASTM D638 | 157 | Mpa | ||
| --1 | ASTM D638 | 8630 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD:-40to40°C | ASTME831 | 5.1E-05 | cm/cm/°C |
| MD:-40to40°C | ASTME831 | 1.4E-05 | cm/cm/°C | |
| 1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 207 | °C | |
| 1.8MPa, unannealed, 3.20mm | ASTM D648 | 204 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | TD | Internal Method | 0.52 | % |
| MD | Internal Method | 0.40 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 100kHz | ASTM D150 | 3.30 | |
| Dissipation factor | 100kHz | ASTM D150 | 3.1E-03 | |
| Dielectric strength | 1.60mm,inOil | ASTM D149 | 31 | KV/mm |
| Volume resistivity | ASTM D257 | 7.6E+16 | ohms·cm | |
| Surface resistivity | ASTM D257 | 2E+13 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.