Material Description
- Material Properties:High toughness|Hydrolysis resistance|Thermal stability|Weather resistance|UV resistance
- Application Areas:Electrical applications|Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| bending strength | 23℃ | ISO 178 | 45 | Mpa |
| Bending modulus | 23℃ | ISO 178 | 1400 | Mpa |
| Tensile modulus | 50mm/min,Yield | ISO 527-2/1A | 6 | % |
| Tensile stress | 50mm/min,Yield | ISO 527-2/1A | 40 | Mpa |
| Tensile modulus | 1mm/min | ISO 527-2/1A | 1500 | Mpa |
| Rockwell hardness | ISO 2039-2 | 101 | M | |
| Impact strength of cantilever beam gap | -30℃ | ISO 180/1A | 10 | KJ/m |
| 23℃ | ISO 180/1A | NB | KJ/m | |
| Charpy Notched Impact Strength | -30℃ | ISO 179/1eA | 10 | KJ/m |
| 23℃ | ISO 179/1eA | 70 | KJ/m | |
| Impact strength of simply supported beam without notch | -30℃ | ISO 179/1eU | NB | KJ/m |
| 23℃ | ISO 179/1eU | NB | KJ/m | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 1.3 | E-4/℃ |
| Melting temperature | ISO 11357-1 | 225 | °C | |
| Glass transition temperature | ISO 11357-1 | 60 | °C | |
| Hot deformation temperature | 1.8Mpa | ISO 75-1/-2 | 48 | °C |
| 0.45Mpa | ISO 75-1/-2 | 110 | °C | |
| Vicat softening temperature | ISO 306 | 130 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23℃,50%相对湿度 | ISO 62 | 0.2 | % |
| 23℃,Saturation | ISO 62 | 0.45 | % | |
| Shrinkage rate | Across Flow | ISO 294-4 | 1.7-2.2 | % |
| Across Flow | ISO 294-4 | 1.7-2.2 | % | |
| Melt Volume Flow Rate (MVR) | ISO 1133 | 9 | CM | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | 1E+14 | Ohm | |
| Dielectric strength | IEC 60243-1 | 24 | KV/mm | |
| Volume resistivity | IEC 60093 | 1E+12 | ohm.m | |
| Dielectric dissipation factor | 1MHz | IEC 60250 | 310 | E-4 |
| Volume resistivity | 100Hz | IEC 60250 | 4.4 | |
| Compared to the Leakage Traceability Index (CTI) | IEC 60112 | 600 | ||
| Dielectric dissipation factor | 100Hz | IEC 60250 | 75 | E-4 |
| Volume resistivity | 1MHz | IEC 60250 | 3.9 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.