PC/ABS Bayblend®  FR-3000 COVESTRO THAILAND

326
  • Unit Price:US$ 2,879 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High mobilityUV resistanceFlame retardant
  • Application Areas:Household appliancesAutomotive sectorElectronic fieldElectrical field
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet Compare

thermal performanceTest ConditionTest MethodTest Result
Heat Deflection TemperatureISO 75-2/B95.0 °C
Heat Deflection TemperatureISO 75-2/A85.0 °C
vicatISO 306/B120103 °C
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-0
UL flame retardant ratingUL 945VB
Limiting Oxygen IndexISO 4589-234 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/12650 Mpa
tensile strengthISO 527-2/5064.0 Mpa
Tensile strainISO 527-2/503.9 %
Nominal tensile fracture strainISO 527-2/5040 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/A30 kJ/m²
Filling analysisTest ConditionTest MethodTest Result
melt viscosityISO 11443-A150 Pa·s
ISO 9660PC+ABS-FR(40)
Physical propertiesTest ConditionTest MethodTest Result
densityISO 11831.18 g/cm³
Melt volume flow rateISO 113320.0 cm3/10min
shrinkage rateISO 25770.40 - 0.60 %
shrinkage rateISO 25770.40 - 0.60 %
Water absorption rateISO 620.40 %
Water absorption rateISO 620.10 %
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityIEC 600931.0E+16 ohms
volume resistivityIEC 600931.0E+16 ohms·cm
relative permittivityIEC 602503.00
relative permittivityIEC 602502.90
injectionTest ConditionTest MethodTest Result
Drying Temperature - Dry Air Dryer80 °C
Drying time - Dry Air Dryer4.0 hr
Suggested maximum moisture content< 0.020 %
Suggested injection volume30 to 70 %
Temperature at the rear of the barrel220 to 230 °C
Temperature in the middle of the barrel225 to 235 °C
Temperature at the front of the material cylinder230 to 240 °C
Spray nozzle temperature255 to 265 °C
Processing (melt) temperature240 to 270 °C
mold temperature60 to 90 °C
Back pressure5.00 to 15.0 Mpa
Exhaust hole depth0.025 to 0.075 mm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.