PBT VALOX™  VX5022 SABIC INNOVATIVE US

264
  • Unit Price:US$ 3,680 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    Guangzhou port, China
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Low warpageAnti deformationFiller: Glass fiber reinforced material20%Filler by weight
  • Application Areas:Automotive components
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Filling analysisTest ConditionTest MethodTest ResultTest Unit
Melt viscosity260°C,1500sec^-1ISO 11443215Pa·s
impact performanceTest ConditionTest MethodTest ResultTest Unit
Dart impact23°C,TotalEnergyASTM D376365.0J
23°CISO 180/1U40kJ/m²
-30°CISO 180/1U35kJ/m²
23°CASTM D4812650J/m
-30°CASTM D4812650J/m
23°CISO 180/1A7.0kJ/m²
0°CISO 180/1A7.0kJ/m²
-30°CISO 180/1A6.0kJ/m²
-30°CISO 179/1eA5.5kJ/m²
-30°CISO 179/2C9.0kJ/m²
23°CISO 179/1eA6.5kJ/m²
23°CISO 179/2C9.0kJ/m²
-30°CISO 179/1eU40kJ/m²
-30°CISO 179/2U50kJ/m²
23°CISO 179/1eU40kJ/m²
23°CISO 179/2U55kJ/m²
-30°CASTM D25680J/m
0°CASTM D25680J/m
23°CASTM D25680J/m
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.60mmUL 94HB
Burning wire flammability index1.00mmIEC 60695-2-12750°C
Burning wire flammability index2.00mmIEC 60695-2-12850°C
Extreme Oxygen IndexISO 4589-223%
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
yieldASTM D6383.0%
yieldISO 527-2/53.0%
crackASTM D6383.0%
crackISO 527-2/53.0%
50.0mm spanASTM D7905800Mpa
--9ISO 1786300Mpa
--10ISO 178150Mpa
Yield, 50.0mm spanASTM D790145Mpa
Fracture bending strainISO 1783.0%
--3ASTM D6387300Mpa
yieldASTM D638125Mpa
yieldISO 527-2/5110Mpa
crackASTM D638125Mpa
crackISO 527-2/5110Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
0.45MPa, unannealed, 64.0mm spanISO 75-2/Bf180°C
0.45MPa, unannealed, 3.20mmASTM D648180°C
Horizontal: -40 to 40 ° CAcross Flow, -40to40℃ASTME8311E-04cm/cm/°C
Horizontal: -40 to 40 ° CAcross Flow, -40to40℃ISO 11359-26.9E-05cm/cm/°C
Horizontal: 23 to 60 ° CAcross Flow, 23to60℃ISO 11359-21E-04cm/cm/°C
Flow: 23 to 150 ° C23to150℃ISO 11359-22.4E-05cm/cm/°C
Horizontal: 23 to 80 ° CAcross Flow, 23to80℃ISO 11359-21E-04cm/cm/°C
Horizontal: 23 to 150 ° CAcross Flow, 23to150℃ISO 11359-21.1E-04cm/cm/°C
1.8MPa, unannealed, 3.20mmASTM D648120°C
1.8MPa, unannealed, 64.0mm span ofISO 75-2/Af120°C
Ball Pressure Test125°CIEC 60695-10-2Pass
Flow: -40 to 40 ° CASTME8314E-05cm/cm/°C
Flow: -40 to 40 ° CISO 11359-22.5E-05cm/cm/°C
Flow: 23 to 60 ° C23to60℃ISO 11359-24E-05cm/cm/°C
Flow: 23 to 80 ° C23to80℃ISO 11359-24E-05cm/cm/°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Shrinkage rateTD2Internal Method0.50-0.90%
Shrinkage rateMD:3.20mmInternal Method0.30-0.50%
Shrinkage rateMD1Internal Method0.30-0.80%
Melt Volume Flow Rate (MVR)265°C/5.0kgISO 113340.0cm3/10min
Melt Volume Flow Rate (MVR)250°C/5.0kgISO 113328.0cm3/10min
Melt Volume Flow Rate (MVR)250°C/2.16kgISO 113313.0cm3/10min
melt mass-flow rate266°C/5.0kgASTM D123850g/10min
melt mass-flow rate265°C/5.0kgASTM D123850g/10min
melt mass-flow rate250°C/2.16kgASTM D123816g/10min
densityASTMD7921.39g/cm³
Water absorption rateSaturation,23°CISO 620.10%
Water absorption rateEquilibrium,23°C,50%RHISO 620.060%
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
50Hz50HzIEC 602503.10
60Hz60HzIEC 602503.10
100Hz100HzIEC 602503.30
1MHz1MHzASTMD1500.014
1MHz1MHzASTMD1503.30
3.20mm, in oilIEC 60243-116KV/mm
1.60mm, in oilIEC 60243-128KV/mm
0.800mm, in oilIEC 60243-131KV/mm
50Hz50HzIEC 602501E-03
60Hz60HzIEC 602501E-03
100Hz100HzIEC 602501E-03
Compared to the anti leakage trace index--IEC 60112PLC 3
Compared to the anti leakage trace indexSolutionBIEC 60112PLC 4
High arc combustion indexHAIUL 746PLC 0
Hot wire ignitionHWIUL 746PLC 0
Surface resistivityIEC 60093>1.0E+15ohms
Volume resistivityASTMD257>1.0E+15ohms·cm
0.800mm,inOilASTM D14931KV/mm
1.60mm,inOilASTM D14928KV/mm
3.20mm, inoilASTM D14916KV/mm
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardnessR-SaleISO 2039-2122
Ball Pressure TestH358/30ISO 2039-1205Mpa
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
Filling materialASTM D22920%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Other Prices

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China