POM DURACON® TR-20 BK JAPAN POLYPLASTIC
287
- Unit Price:US$ 3,300 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:77MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:enhance|High rigidity
- Application Areas:Automotive sector|Industrial machinery|Electronic field|Electrical field
- Color:--
- Grade:Enhanced level
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 4100 | Mpa | |
| Tensile strain | Break | ISO 527-2 | 5.0 | % |
| tensile strength | ISO 527-2 | 59.0 | Mpa | |
| Tensile modulus | ISO 527-2 | 4500 | Mpa | |
| Wear factor | 0.49MPa,0.30m/sec7 | JISK7218 | 8000 | 10^-8mm³/N·m |
| 0.060MPa,0.15m/sec6 | JISK7218 | 7000 | 10^-8mm³/N·m | |
| 0.060MPa,0.15m/sec5 | JISK7218 | 500 | 10^-8mm³/N·m | |
| Friction coefficient | Steel - Dynamic3 | JISK7218 | 0.56 | |
| Dynamic2 | JISK7218 | 0.34 | ||
| bending strength | ISO 178 | 96.0 | Mpa | |
| Wear factor | 0.49MPa,0.30m/sec4 | JISK7218 | 150 | 10^-8mm³/N·m |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD:23to55°C | Internal Method | 8E-05 | cm/cm/°C |
| MD:23to55°C | Internal Method | 8E-05 | cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 125 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.50 | % |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 16.0 | cm3/10min |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 21 | g/10min |
| density | ISO 1183 | 1.53 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 3.00mm | IEC 60243-1 | 21 | KV/mm |
| Surface resistivity | IEC 60093 | 9E+15 | ohms | |
| Volume resistivity | IEC 60093 | 2E+14 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Scale | ISO 2039-2 | 75 | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| ColourNumber | CF2001/CD3501 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.