PC LEXAN™ HPS6 SABIC INNOVATIVE US
192
- Unit Price:US$ 9,081 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility
- Application Areas:medical care|medicine
- Color:--
- Grade:Light diffusion level
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 15 | kJ/m² |
| 23°C | ISO 179/1eA | 75 | kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | NoBreak | |
| 23°C | ISO 179/1eU | NoBreak | ||
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 10 | kJ/m² |
| 23°C | ISO 180/1A | 70 | kJ/m² | |
| Suspended wall beam without notch impact strength | -30°C | ISO 180/1U | NoBreak | |
| 23°C | ISO 180/1U | NoBreak | ||
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 65.0 | J |
| 23°C,TotalEnergy | ASTM D3763 | 65.0 | J | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| elongation | Break | ASTM D638 | 140 | % |
| Tensile strain | Yield | ISO 527-2/50 | 6.0 | % |
| elongation | Yield | ASTM D638 | 6.5 | % |
| tensile strength | Break | ISO 527-2/50 | 75.0 | Mpa |
| Break | ASTM D638 | 68.9 | Mpa | |
| Yield | ISO 527-2/50 | 60.0 | Mpa | |
| Yield | ASTM D638 | 62.1 | Mpa | |
| Tensile modulus | ISO 527-2/1 | 2300 | Mpa | |
| ASTM D638 | 2310 | Mpa | ||
| Tensile strain | Break | ISO 527-2/50 | 140 | % |
| Bending modulus | 50.0mmSpan | ASTM D790 | 2340 | Mpa |
| ISO 178 | 2250 | Mpa | ||
| bending strength | ISO 178 | 95.0 | Mpa | |
| Yield,50.0mmSpan | ASTM D790 | 97.9 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ASTM D152511 | 154 | °C | |
| -- | ISO 306/B50 | 143 | °C | |
| -- | ISO 306/B120 | 140 | °C | |
| Ball Pressure Test | 75°C | IEC 60695-10-2 | Pass | |
| Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 124 | °C |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 132 | °C | |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 124 | °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 138 | °C | |
| Linear coefficient of thermal expansion | TD:-40to40°C | ISO 11359-2 | 6E-05 | cm/cm/°C |
| TD:-40to40°C | ASTME831 | 5.7E-05 | cm/cm/°C | |
| MD:-40to40°C | ASTME831 | 6.2E-05 | cm/cm/°C | |
| MD:-40to40°C | ISO 11359-2 | 6E-05 | cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed,3.20mm | ASTM D648 | 135 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 | % |
| Saturation,23°C | ISO 62 | 0.35 | % | |
| 24hr | ASTM D570 | 0.15 | % | |
| Shrinkage rate | TD:3.20mm | Internal Method | 0.50-0.70 | % |
| MD:3.20mm | Internal Method | 0.50-0.70 | % | |
| MD:--2 | Internal Method | 0.50-0.70 | % | |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 6.50 | cm3/10min |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 110 | g/10min |
| 300°C/1.2kg | ASTM D1238 | 7.0 | g/10min | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 118 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.