TPV Santoprene™ 8201-60 CELANESE USA

186
  • Unit Price:US$ 4,649 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    18MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Low friction coefficientLow mold expansionRecyclable materialsControllable mold expansionCleanableGood melt strengthGood colorabilityOzone resistanceChemical resistanceLow water absorptionNot absorbing water
  • Application Areas:Kitchen utensilsHome appliance componentsFatigue relief suppliesSoft handleSmart phoneMonitorPhoneHome appliance componentsFatigue relief suppliesSoft handleKitchen utensilsMonitor
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

hardnessTest ConditionTest MethodTest Result
Shore hardness邵氏A,15秒,23°CISO 86864
thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTM D746-60.0 °C
brittle temperatureISO 812-60.0 °C
RTI ElecUL 746100 °C
RTI Str1.1mmUL 74690.0 °C
RTI Str1.6mmUL 74690.0 °C
RTI Str3.0mmUL 74695.0 °C
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating1.1mmUL 94HB
UL flame retardant rating1.6mmUL 94HB
UL flame retardant rating3.0mmUL 94HB
elastomerTest ConditionTest MethodTest Result
tear strength23°C,Across Flow (横向)ISO 34-132 kN/m
compression set70°C,22hrASTM D395B29 %
compression set70°C,22hrISO 81529 %
Tensile stress100%应变,23°C,横向流量ASTM D4122.20 Mpa
Tensile stress100%应变,23°C,横向流量ISO 372.20 Mpa
tensile strength断裂,23°C,横向流量ASTM D4125.90 Mpa
tensile strengthBreak,23°CISO 375.90 Mpa
elongation断裂,23°C,横向ASTM D412520 %
elongation断裂,23°C,横向ISO 37520 %
tear strength23°C,横向流量ASTM D62432.0 kN/m
agingTest ConditionTest MethodTest Result
Change rate of tensile strength in air150°C,168hrASTM D573-9.0 %
Change rate of tensile strength in air150°C,168hrISO 188-9.0 %
Change rate of ultimate elongation in air150°C,168hrASTM D573-7.0 %
Hardness change rate in the airShoreA,150°C,168hrASTM D5731.0
Shore hardnessShoreA,150°C,168hrISO 1881.0
Changes in air quality150°C,168hrASTM D573-8.0 %
Changes in air quality150°C,168hrISO 188-8.0 %
Change rate of tensile strength in air23°C,168hr,inIRM903OilASTM D471-17 %
Change rate of tensile strength in air23°C,168hr,inSodiumChloride,15%ASTM D471-4.0 %
Change rate of ultimate elongation in air23°C,168hr,inSodiumHydroxide,50%ASTM D471-2.0 %
Change rate of ultimate elongation in air23°C,168hr,inSulfuricAcid,98%ASTM D4715.0 %
Change rate of ultimate elongation in air23°C,168hr,在水中ASTM D47111 %
Tensile stress change rate23°C,168hr,inIRM903Oil,断裂ISO 1817-21 %
Tensile stress change rate23°C,168hr,inSodiumChloride,15%,断裂ISO 1817-5.0 %
Tensile stress change rate23°C,168hr,inSodiumHydroxide,50%,断裂ISO 1817-2.0 %
Tensile stress change rate23°C,168hr,inSulfuricAcid,98%,断裂ISO 18175.0 %
Tensile stress change rate23°C,168hr,在水中,断裂ISO 181711 %
Change rate of hardness (Shore) in the airShoreA,23°C,168hr,inIRM903OilASTM D471-13
Change rate of hardness (Shore) in the airShoreA,23°C,168hr,inSodiumChloride,15%ASTM D4712.0
Change rate of tensile strength in air23°C,168hr,inSodiumHydroxide,50%ASTM D471-2.0 %
Change rate of tensile strength in air23°C,168hr,inSulfuricAcid,98%ASTM D4713.0 %
Change rate of tensile strength in air23°C,168hr,在水中ASTM D471-3.0 %
Change rate of tensile strength in air23°C,168hr,inIRM903OilISO 1817-17 %
Change rate of tensile strength in air23°C,168hr,inSodiumChloride,15%ISO 1817-4.0 %
Change rate of tensile strength in air23°C,168hr,inSodiumHydroxide,50%ISO 1817-2.0 %
Change rate of tensile strength in air23°C,168hr,inSulfuricAcid,98%ISO 18173.0 %
Change rate of tensile strength in air23°C,168hr,在水中ISO 1817-3.0 %
Change rate of ultimate elongation in air23°C,168hr,inIRM903OilASTM D471-21 %
Change rate of ultimate elongation in air23°C,168hr,inSodiumChloride,15%ASTM D471-5.0 %
Change rate of hardness (Shore) in the airShoreA,23°C,168hr,inSodiumHydroxide,50%ASTM D4712.0
Change rate of hardness (Shore) in the airShoreA,23°C,168hr,inSulfuricAcid,98%ASTM D471-1.0
Change rate of hardness (Shore) in the airShoreA,23°C,168hr,inWaterASTM D4710.0
Shore hardnessShoreA,23°C,168hr,inIRM903OilISO 1817-13
Shore hardnessShoreA,23°C,168hr,inSodiumChloride,15%ISO 18172.0
Shore hardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ISO 18172.0
Shore hardnessShoreA,23°C,168hr,inSulfuricAcid,98%ISO 1817-1.0
Shore hardnessShoreA,23°C,168hr,inWaterISO 18170.0
mass change fraction23°C,168hr,inIRM903OilASTM D47147 %
mass change fraction23°C,168hr,inSodiumChloride,15%ASTM D4710.0 %
mass change fraction23°C,168hr,inSodiumHydroxide,50%ASTM D4710.0 %
mass change fraction23°C,168hr,inSulfuricAcid,98%ASTM D4710.0 %
mass change fraction23°C,168hr,在水中ASTM D4710.0 %
mass change fraction23.0°C,168hr,inSodiumHydroxide,50%ISO 18170.0 %
mass change fraction23.0°C,168hr,inSulfuricAcid,98%ISO 18170.0 %
mass change fraction23.0°C,168hr,inSodiumChloride,15%ISO 18170.0 %
mass change fraction23.0°C,168hr,inIRM903OilISO 181747 %
Electrical performanceTest ConditionTest MethodTest Result
Hot wire ignition (HWI)1.6mmUL 746PLC 3
Hot wire ignition (HWI)3.0mmUL 746PLC 2
Compared to the Leakage Tracking Index (CTI)CTIUL 746PLC 0
High arc combustion index (HAI)HAIUL 746PLC 0
High Voltage Arc Traceability Rate (HVTR)PLCUL 746
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us

Get App

Top