Material Description
- Material Properties:heat-resisting|High temperature resistance|High impact resistance|High mobility|Flame retardant
- Application Areas:Household appliances|Automotive sector|Electronic field|Electrical field
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 54.2 | J |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.76mm | UL 94 | V-2 | |
| 1.5mm | UL 94 | V-0 | ||
| 2.5mm | UL 94 | 5VB | ||
| 3.4mm | UL 94 | 5VA | ||
| Extreme Oxygen Index | ASTM D2863 | 30 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | Yield,100mmSpan | ASTM D790 | 96.5 | Mpa |
| Bending modulus | 100mmSpan | ASTM D790 | 2590 | Mpa |
| elongation | Break | ASTM D638 | 40 | % |
| tensile strength | Yield | ASTM D638 | 64.1 | Mpa |
| elongation | Yield | ASTM D638 | 5.0 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| RTI Str | UL 746 | 85.0 | °C | |
| RTI Imp | UL 746 | 85.0 | °C | |
| RTI Elec | UL 746 | 85.0 | °C | |
| thermal conductivity | ASTMC177 | 0.20 | W/m/K | |
| Linear coefficient of thermal expansion | TD:-30to30°C | ASTM D696 | 7.2E-05 | cm/cm/°C |
| MD:-30to30°C | ASTM D696 | 7.2E-05 | cm/cm/°C | |
| Vicat softening temperature | ASTM D15254 | 113 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 93.3 | °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 87.8 | °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 102 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 260°C/2.16kg | ASTM D1238 | 22 | g/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.40-0.60 | % |
| TD:3.20mm | Internal Method | 0.40-0.60 | % | |
| Water absorption rate | 24hr | ASTM D570 | 0.10 | % |
| Equilibrium,23°C | ASTM D570 | 0.40 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot wire ignition | HWI | UL 746 | PLC 2 | |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 3 | |
| High arc combustion index | HAI | UL 746 | PLC 0 | |
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 2 | |
| Arc resistance | ASTM D495 | PLC6 | ||
| Dissipation factor | 1MHz | ASTM D150 | 7.1E-03 | |
| 60Hz | ASTM D150 | 5.2E-03 | ||
| 50Hz | ASTM D150 | 5.2E-03 | ||
| Dielectric constant | 1MHz | ASTM D150 | 2.70 | |
| 60Hz | ASTM D150 | 2.80 | ||
| Surface resistivity | ASTM D257 | >1.0E+16 | ohms | |
| Volume resistivity | ASTM D257 | 1.6E+17 | ohms·cm | |
| Dielectric strength | 3.20mm,inOil | ASTM D149 | 24 | KV/mm |
| Dielectric constant | 50Hz | ASTM D150 | 2.80 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 121 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Other Prices
| Supplier | Unit Price |
|---|---|