PC TRIREX® 3022U SAMYANG KOREA
208
- Unit Price:US$ 3,059 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:15MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|transparent
- Application Areas:Automotive sector|Electronic field|Electrical field
- Color:--
- Grade:Weather resistant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ASTM D1238 | 16 g/10 min | |
Water absorption rate | ASTM D570 | 0.15 % |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTM D1003 | 0.40 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-2 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D638 | 69.0 Mpa | |
elongation | ASTM D638 | 130 % | |
Flexural modulus | ASTM D790 | 2250 Mpa | |
bending strength | ASTM D790 | 93.0 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | ASTM D257 | 4.0E+16 ohms·cm | |
dielectric strength | ASTM D149 | 30 KV/mm | |
arc resistance | ASTM D495 | 120 sec |
injection | Test Condition | Test Method | Test Result |
---|---|---|---|
drying temperature | 120 °C | ||
drying time | 3.0 to 5.0 hr | ||
Suggested maximum moisture content | 0.020 % | ||
Temperature at the rear of the barrel | 235 to 260 °C | ||
Temperature in the middle of the barrel | 250 to 275 °C | ||
Temperature at the front of the material cylinder | 265 to 290 °C | ||
Spray nozzle temperature | 265 to 300 °C | ||
Processing (melt) temperature | 265 to 300 °C | ||
Temperature | 65 to 105 °C | ||
Back pressure | 0.250 to 0.700 Mpa | ||
screw speed | 40 to 70 rpm | ||
Exhaust hole depth | 0.020 to 0.080 mm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 134 °C | |
Linear coefficient of thermal expansion | ASTM D696 | 5.0E-5 - 7.0E-5 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.