plas

MABS WANOVATE® T126 YANTAI WANHUA

34
  • Unit Price:US$ 2,045 /MT
  • Packaging Specification:
  • Supply Quantity:
    32MT
  • Delivery Terms:
    DDP
  • :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High transparency
  • Application Areas:--
  • Color:High transparency
  • Grade:Injection grade, extrusion grade, optical grade, infrared penetration grade

Material Certification

TDS

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
turbidity3mmASTMD10033.71 %
Transmittance rate3mmASTMD100388.5 %
Refractive indexASTMD5421.518±0.003
CONDITIONTest ConditionTest MethodTest Result
drying temperature70-80
drying time3-4 h
The first temperature segment200-210
Second stage temperature210-220
Third stage temperature210-220
Nozzle temperature200-210
Melting temperature200-250
Optimal melting temperature220
Mold temperature40-80
Screw speed0.05-0.2 m/s
Recommended injection volume30-70 %
Back pressure2-10 bar
Holding pressure50-75 %
mechanical propertiesTest ConditionTest MethodTest Result
tensile strength50mm/minASTM D63845 MPa
Tensile modulus1mm/minASTMD6382330 MPa
Yield stress50mm/min,屈服ASTMD63845 MPa
Elongation at Break50mm/minASTMD63816 %
bending strength10mm/minASTMD79069 MPa
Bending modulus10mm/minASTMD7902230 MPa
Izod Notched Impact Strength23°℃ASTM D256135 J/m
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature (unannealed)1.82MPa;6.4mm,未退火ASTMD64881.3
Vicat softening temperature120°C/h:50NASTMD152588.8
combustion performanceTest ConditionTest MethodTest Result
Flame retardant grade1.2mmUL94HB
Physical propertiesTest ConditionTest MethodTest Result
Melt index220°C/10KaASTMD123823 g/10min
Molding shrinkage rateASTMD9550.4-0.7
densityASTMD7921.10 g/cm3
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.