Material Description

  • Material Properties:High temperature resistanceFlame retardantGlass fiber reinforcedenhancewear resistantFiller: Glass fiber reinforced material40% filler by weight
  • Application Areas:Fitness equipmentHousehold appliancesElectrical/Electronic Applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strengthISO 18040 kJ/m²
Suspended wall beam without notch impact strength3.18mmASTM D4812750 J/m
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating1.6mmUL 94V-0
Extreme Oxygen IndexASTM D286348 %
mechanical propertiesTest ConditionTest MethodTest Result
Wear factorASTM D37021.6E-06 m/hr
Friction coefficientvs.Steel-DynamicASTM D37020.32
Poisson's ratio0.40
compressive strengthASTM D695255 Mpa
bending strengthISO 178280 Mpa
bending strengthASTM D790269 Mpa
Bending modulusISO 17814000 Mpa
Bending modulusASTM D79014500 Mpa
Tensile strainBreakISO 527-21.6 %
elongationBreakASTM D6381.6 %
tensile strengthISO 527-2190 Mpa
tensile strengthASTM D638186 Mpa
thermal performanceTest ConditionTest MethodTest Result
UL temperature ratingUL 746B180 °C
Linear coefficient of thermal expansionTD:导热系数ASTME8310.33 W/m/K
Linear coefficient of thermal expansionTD:100to200°CASTME8318E-05 cm/cm/°C
Linear coefficient of thermal expansionTD:-50to50°CASTME8314E-05 cm/cm/°C
Linear coefficient of thermal expansionMD:100to200°CASTME8311E-05 cm/cm/°C
Linear coefficient of thermal expansionMD:-50to50°CASTME8311.5E-05 cm/cm/°C
Hot deformation temperature1.8MPa,UnannealedASTM D648265 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateMD:3.20mm0.20 %
Shrinkage rateTD:3.20mm0.50 %
Water absorption rate23°C,24hrASTM D5700.020 %
Electrical performanceTest ConditionTest MethodTest Result
Dielectric strengthASTM D14922 KV/mm
Volume resistivityASTM D2571E+16 ohms·cm
Surface resistivityASTM D2571E+16 ohms
Dielectric constant25°C,1kHzASTM D1503.70
Dielectric constant25°C,1MHzASTM D1503.70
Dissipation factor25°C,1kHzASTM D1502E-03
Dissipation factor25°C,1MHzASTM D1503E-03
Compared to the anti leakage trace indexCTIUL 746PLC 4
insulation resistance90°C1E+11 ohms
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessM-SaleASTM D78597
Rockwell hardnessR-SaleASTM D785117
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.