POM Ultraform® N2720M63 BASF GERMANY
320
- Unit Price:US$ 2,730 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:43.8MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High toughness|Filler: Mineral filler|30%|Filler by weight
- Application Areas:Toy|Automotive Applications
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 55 | kJ/m² |
| 23°C | ISO 179/1eU | 55 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.5 | kJ/m² |
| -30°C | ISO 179/1eA | 3.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Flammability level | 1.6mm | IEC 60695-11-10,-20 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile creep modulus | 1000hr | ISO 899-1 | 2750 | Mpa |
| Nominal tensile fracture strain | ISO 527-2/50 | 6.0 | % | |
| Tensile strain | Yield | ISO 527-2/50 | 5.0 | % |
| tensile strength | Yield | ISO 527-2/50 | 75.0 | Mpa |
| Tensile modulus | ISO 527-2 | 7000 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Maximum operating temperature | 短周期操作 | 110 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 140 | °C |
| Melting temperature | ISO 11357-3 | 166 | °C | |
| Linear coefficient of thermal expansion | MD:23to55°C | ISO 11359-2 | 4.5E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 | % |
| Saturation,23°C | ISO 62 | 0.90 | % | |
| Shrinkage rate | MD | ISO 294-4 | 1.2 | % |
| TD | ISO 294-4 | 1.5 | % | |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 3.80 | cm3/10min |
| Apparent density | 0.85 | g/cm³ | ||
| density | ISO 1183 | 1.65 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 | |
| Dissipation factor | 1MHz | IEC 60250 | 5E-03 | |
| Relative permittivity | 1MHz | IEC 60250 | 4.20 | |
| Dielectric strength | IEC 60243-1 | 85 | KV/mm | |
| Volume resistivity | IEC 60093 | 1E+14 | ohms·cm | |
| Surface resistivity | IEC 60093 | 1E+14 | ohms | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | H961/30 | ISO 2039-1 | 190 | Mpa |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| ISOType | ISO 9988-1 | POM-K.M-GNR.02-003.M30 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.