Material Description
- Material Properties:High impact resistance|Low odor and no taste
- Application Areas:switch|Fasteners
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 130 | J/m |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 13 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.8mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | 23°C | ISO 178 | 55.0 | Mpa |
| 23°C | ASTM D790 | 60.0 | Mpa | |
| Bending modulus | 23°C | ISO 178 | 1900 | Mpa |
| 23°C | ASTM D790 | 1800 | Mpa | |
| elongation | Break,23°C | ISO 527-2 | >50 | % |
| Yield,23°C | ASTM D638 | 140 | % | |
| tensile strength | 23°C | ISO 527-2 | 45.0 | Mpa |
| Yield,23°C | ASTM D638 | 45.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 1.3E-04 | cm/cm/°C |
| Melting temperature | ISO 11357-3 | 166 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 72.0 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 82.0 | °C | |
| 0.45MPa,Unannealed | ASTM D648 | 145 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD | ASTM D955 | 1.7 | % |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 7.5 | g/10min |
| 190°C/2.16kg | ASTM D1238 | 12 | g/10min | |
| density | ASTMD792 | 1.36 | g/cm³ | |
| Shrinkage rate | TD | ISO 294-4 | 2.2 | % |
| MD | ISO 294-4 | 2.0 | % | |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.63 | % |
| Equilibrium,23°C,60%RH | ASTM D570 | 0.25 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 1MHz | ASTM D150 | 6E-03 | |
| Dielectric constant | ASTM D150 | 3.70 | ||
| Dielectric strength | ASTMD149 | 19 | KV/mm | |
| Volume resistivity | ASTMD257 | 1E+14 | ohms·cm | |
| Surface resistivity | ASTMD257 | 1E+16 | ohms | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Scale | ASTM D785 | 76 | |
| M-Sale | ISO 2039-2 | 83 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.