PA12 VESTAMID® L-GF15 EVONIK GERMANY
4
- Unit Price:US$ 29,000 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Plastic bag
- Supply Quantity:10MT
- Delivery Terms:CIF
- Destination Port :Saigon port, Vietnam
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
Shenzhen Benia New Materials Technology Co., Ltd.
+86 1560********View
tnni********View
For more details, please contact the supplier!
Material Description
- Material Properties:Low temperature impact resistance|Resistance to stress cracking|Fatigue resistance
- Application Areas:Cable sheath|Automotive Applications
- Color:--
- Grade:Extrusion grade
Material Certification

Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 0.65 % | |
ISO 294-4 | 0.35 % | ||
Water absorption rate | ISO 62 | 1.3 % | |
ISO 62 | 0.60 % | ||
density | ISO 1183 | 1.12 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB | |
UL 94 | V-2 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO Shortcut | ISO 1874 | PA12.MHR.16-050.GF15 | |
electrolytic corrosion | IEC 60426 | A1 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strain | ISO 527-2 | 6.0 % | |
Tensile modulus | ISO 527-2 | 3900 Mpa | |
tensile strength | ISO 527-2 | 95.0 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 11 kJ/m² | |
ISO 179/1eA | 17 kJ/m² | ||
Impact strength of simply supported beam without notch | ISO 179/1eU | 75 kJ/m² | |
ISO 179/1eU | 80 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Dissipation Factor | IEC 60250 | 0.026 | |
IEC 60250 | 0.038 | ||
relative permittivity | IEC 60250 | 4.00 | |
IEC 60250 | 3.40 | ||
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
dielectric strength | IEC 60243-1 | 44 KV/mm | |
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | V | |
IEC 60112 | V |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/B | 175 °C | |
ISO 75-2/A | 160 °C | ||
melting temperature | ISO 11357-3 | 178 °C | |
vicat | ISO 306/A | 175 °C | |
ISO 306/B | 170 °C | ||
Linear coefficient of thermal expansion | ISO 11359-2 | 8E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.