TPV Santoprene™ 8211-55 CELANESE USA
19
- Unit Price:US$ 6,750 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Guangzhou Hushang Chemical Co., Ltd
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:dimensional stability |Low friction coefficient|Recyclable materials|Cleanable|Good forming performance|Good colorability|High mobility|Ozone resistance|Chemical resistance|soft|Low water absorption|Not absorbing water
- Application Areas:packing|Automotive sector|Soft handle|Smart phone|Consumer goods sector|Consumer product application field|packing|Soft handle|Phone|Application in the automotive field
- Color:--
- Grade:Weather resistant grade
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| UL flame retardant rating | 1.1mm | UL 94 | HB | |
| 3.0mm | UL 94 | HB | ||
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
| Tensile stress | 100%Strain,23°C,横向Flow | ASTMD412 | 2.10 | Mpa |
| tensile strength | Break,23°C,横向Flow | ASTMD412 | 4.60 | Mpa |
| elongation | Break,23°C,Across Flow | ASTMD412 | 480 | % |
| Permanent compression deformation | 70°C,22hr3 | ASTM D395B | 19 | % |
| 125°C,70hr3 | ASTM D395B | 49 | % | |
| 70°C,22hr4 | ISO 815 | 19 | % | |
| 125°C,70hr4 | ISO 815 | 49 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Brittle temperature | ASTMD746 | -62.0 | °C | |
| RTI Elec | UL 746 | 100 | °C | |
| RTI | 1.1mm | UL 746 | 90.0 | °C |
| 3.0mm | UL 746 | 95.0 | °C | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA,15Sec,23°C | ISO 868 | 59 | |
| aging | Test Condition | Test Method | Test Result | Test Unit |
| Change rate of tensile strength in air | 150°C,168hr | ASTMD573 | -11 | % |
| Change rate of ultimate elongation in air | 150°C,168hr | ASTMD573 | -10 | % |
| Change rate of hardness (Shore) in the air | ShoreA,150°C,168hr | ASTMD573 | 1.0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.