PBT 2002-2 CELANESE USA
246
- Unit Price:US$ 3,182 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:33MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Processability|Moderate liquidity|Lubricity|currency
- Application Areas:currency
- Color:--
- Grade:--
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -30℃ | ISO 179/1eU | 190 KJ/m |
| 23℃ | ISO 179/1eU | NB KJ/m | |
| bending strength | 23℃ | ISO 178 | 80 Mpa |
| Bending modulus | 23℃ | ISO 178 | 2500 Mpa |
| tensile strength | ISO 527-2/1A | 60 Mpa | |
| Tensile modulus | 50mm/min,Yield | ISO 527-2/1A | 4 % |
| Tensile stress | 50mm/min,Yield | ISO 527-2/1A | 60 Mpa |
| Tensile modulus | 1mm/min | ISO 527-2/1A | 2600 Mpa |
| Rockwell hardness | ISO 2039-2 | 78 M | |
| Impact strength of cantilever beam gap | 23℃ | ISO 180/1A | 5.0 KJ/m |
| Charpy Notched Impact Strength | -30℃ | ISO 179/1eA | 6 KJ/m |
| 23℃ | ISO 179/1eA | 6 KJ/m |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8Mpa | ISO 75-1/-2 | 55 °C |
| 0.45Mpa | ISO 75-1/-2 | 150 °C | |
| Glass transition temperature | ISO 11357-1 | 60 °C | |
| Melting temperature | ISO 11357-1 | 225 °C | |
| Vicat softening temperature | ISO 306 | 190 °C | |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 1.1 E-4/℃ |
| Across Flow | ISO 11359-2 | 1.27 E-4/℃ | |
| UL flame retardant rating | UL 94 | HB |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Extreme Oxygen Index | ISO 4589 | 22 % | |
| Water absorption rate | 23℃,Saturation | ISO 62 | 0.09 % |
| density | ISO 1183 | 1310 kg/m | |
| Melt Volume Flow Rate (MVR) | ISO 1133 | 20 CM | |
| Shrinkage rate | ISO 294-4 | 1.8-2.0 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the Leakage Traceability Index (CTI) | IEC 60112 | 600 | |
| Dielectric strength | IEC 60243-1 | 23 KV/mm | |
| Surface resistivity | IEC 60093 | 1E+15 Ohm | |
| Volume resistivity | IEC 60093 | 1E+13 ohm.m | |
| Dielectric dissipation factor | 1MHz | IEC 60250 | 220 E-4 |
| 100Hz | IEC 60250 | 14 E-4 | |
| Volume resistivity | 1MHz | IEC 60250 | 3.5 |
| 100Hz | IEC 60250 | 4 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.