TPU Desmopan® 1485A COVESTRO GERMANY
209
- Unit Price:US$ 5,132 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:31.6MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:corrugated pipe|Hose|Joint|Engineering accessories
- Color:--
- Grade:Extrusion grade
Technical Data Sheet
| other | Test Condition | Test Method | Test Result |
|---|---|---|---|
| characteristic | 挤出和注射牌号.适合于吹塑成型.极宽的加工范围。 | ||
| purpose | 波纹管.软管.非增强产品、型材、工程注射产品。 |
| machinability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Mold temperature | 20 °C | ||
| Melt Temperature | 200-220 °C |
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Resilience | ISO 4662 | 44 % | |
| Permanent compression deformation | 70°C, 24 hr5 | ISO 815 | 29 % |
| 70°C, 24 hr3 | ISO 815 | 40 % | |
| 23°C, 72 hr | ISO 815 | 19 % | |
| tear strength | 23°C | ISO 34-1 | 63 kN/m |
| squeeze out | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Temperature | 200 to 220 °C | ||
| drying temperature | < 80 °C |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ASTM D2240/ISO 868 | 86 Shore A | |
| ASTM D2240/ISO 868 | 33 Shore D | ||
| tear strength | ASTM D624/ISO 34 | 78 n/mm² | |
| Tensile modulus | 300% | ASTM D412/ISO 527 | 9 Mpa/Psi |
| Wear resistance | ISO 4649 | 30.0 mm³ | |
| Tensile storage modulus | 60°C | ISO 6721 | 21.0 Mpa |
| 20°C | ISO 6721 | 31.0 Mpa | |
| -20°C | ISO 6721 | 290 Mpa | |
| Tensile strain | Break, 23°C | DIN 53504 | 700 % |
| tensile strength | 300% Strain, 23°C | DIN 53504 | 9.00 Mpa |
| 100% Strain, 23°C | DIN 53504 | 5.20 Mpa | |
| Break, 23°C | DIN 53504 | 45.0 Mpa | |
| Resilience | ASTM D2630/ISO 4662 | 46 % | |
| Tensile modulus | 100% | ASTM D412/ISO 527 | 5 Mpa/Psi |
| Wear and tear loss | ISO 4649 | 19 mm³ | |
| Permanent compression deformation | ISO 815 | 36 % | |
| ISO 815 | 11 % |
| injection | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Processing (melt) temperature | 220 to 240 °C | ||
| drying temperature | < 80 °C | ||
| Mold temperature | 20 °C |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | Shore D, 1 Sec, 23°C | ISO 7619 | 33 |
| Shore A, 1 Sec, 23°C | ISO 7619 | 84 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.