ECTFE HALAR® 901 SOLVAY USA
335
- Unit Price:US$ 49,287 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | -40°C,3.20mm | ASTM D256 | 210 J/m |
23°C,3.20mm | ASTM D256 | 无断裂 |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-0 | |
Extreme Oxygen Index | ASTM D2863 | 52 % |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Friction coefficient | 泰伯耐磨性(1000Cycles,500g,CS-17Wheel) | ASTM D1894 | 5.00 mg |
Tensile modulus | 23°C | ASTM D638 | 1660 Mpa |
tensile strength | Yield,23°C | ASTM D638 | 30.0 Mpa |
Break,23°C | ASTM D638 | 54.0 Mpa | |
elongation | Yield,23°C | ASTM D638 | 5.0 % |
Break,23°C | ASTM D638 | 250 % | |
Bending modulus | 23°C | ASTM D790 | 1690 Mpa |
bending strength | 23°C | ASTM D790 | 47.0 Mpa |
Friction coefficient | Itself - Dynamic | ASTM D1894 | 0.20 |
Itself - Static | ASTM D1894 | 0.20 |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 90.0 °C |
1.8MPa,Unannealed | ASTM D648 | 65.0 °C | |
Brittle temperature | ASTM D746A | <-76.0 °C | |
Glass transition temperature | DMA | 85.0 °C | |
Melting temperature | ASTM D3418 | 242 °C | |
Crystallization peak temperature | DSC | ASTM D3418 | 222 °C |
Linear coefficient of thermal expansion | MD | ASTM D696 | 1E-04 cm/cm/°C |
specific heat | 23°C | ASTM D3418 | 962 J/kg/°C |
thermal conductivity | 40°C | ASTMC177 | 0.15 W/m/K |
Crystallization peak temperature | ASTM D3418 | 40.0 J/g | |
Thermal stability -1% mass loss, N | TGA | 405 °C | |
Fusion temperature | ASTM D3418 | 42.0 J/g |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.68 g/cm³ | |
melt mass-flow rate | 275°C/2.16kg | ASTM D1238 | 0.90to1.3 g/10min |
Shrinkage rate | MD | ASTM D955 | 2.5 % |
Water absorption rate | Equilibrium | ASTM D570 | <0.10 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | 23°C | ASTM D257 | 5.5E+16 ohms·cm |
Dielectric strength | 23°C,3.20mm | ASTM D149 | 14 KV/mm |
Dielectric constant | 23°C,1MHz | ASTM D150 | 2.57 |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | R-Scale | ASTM D785 | 90 |
Shore hardness | ShoreD | ASTM D2240 | 75 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.