230
- Unit Price:US$ 5,536 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Dimensional stability|Ozone resistant|Recyclable|Low tenderness|Oil resistant
- Application Areas:Industrial applications|Automotive Applications|Application in the automotive field
- Color:--
- Grade:Injection grade
Technical Data Sheet
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
elongation | Break,23°C,Across Flow | ISO 37 | 290 % |
tear strength | 23°C,横向Flow | ASTM D624 | 30.0 kN/m |
elongation | Break,23°C,Across Flow | ASTM D412 | 290 % |
tensile strength | Break,23°C | ISO 37 | 8.80 Mpa |
Break,23°C,横向Flow | ASTM D412 | 8.80 Mpa | |
Tensile stress | 100%Strain,23°C,横向Flow | ISO 37 | 5.20 Mpa |
100%Strain,23°C,横向Flow | ASTM D412 | 5.20 Mpa | |
Permanent compression deformation | 125°C,70hr | ISO 815 | 47 % |
70°C,22hr | ISO 815 | 30 % | |
125°C,70hr | ASTM D395B | 47 % | |
70°C,22hr | ASTM D395B | 30 % | |
tear strength | 23°C,Across Flow (Across Flow) | ISO 34-1 | 30 kN/m |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Brittle temperature | ISO 812 | -32.0 °C | |
ASTM D746 | -32.0 °C |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ShoreA,15Sec,23°C | ISO 868 | 83 |
aging | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume change | 125°C,70hr,在IRM903油中 | ISO 1817 | 4.0 % |
125°C,70hr,在IRM903油中 | ASTM D471 | 4.0 % | |
Change rate of ultimate elongation in air | 125°C,70hr,inIRM903Oil | ISO 1817 | -48 % |
Elongation at Break | 125°C,70hr,inIRM903Oil | ASTM D471 | -48 % |
Tensile strain change rate | 125°C,70hr,inIRM903Oil | ISO 1817 | -38 % |
Change rate of tensile strength in air | 125°C,70hr,inIRM903Oil | ASTM D471 | -38 % |
Shore hardness | ShoreA,125°C,168hr | ISO 188 | 2.0 |
Hardness change rate in the air | ShoreA,125°C,168hr | ASTM D573 | 2.0 |
Elongation at Break | 125°C,168hr | ASTM D573 | -37 % |
Change rate of tensile strength in air | 125°C,168hr | ISO 188 | 6.0 % |
125°C,168hr | ASTM D573 | 6.0 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.