PC/PET XYLEX™ X7200MR-NA9A002 SABIC INNOVATIVE US
10
- Unit Price:US$ 2,090 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Guangdong Renhong New Material Co., Ltd.
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|High heat resistance
- Application Areas:Automotive Applications|Electronic and electrical accessories
- Color:--
- Grade:Injection grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | ISO 489 | 1.557 | ||
| transmissivity | 2540μm | ASTM D1003 | 88.0 | % |
| turbidity | 2540μm | ASTM D1003 | 1.1 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 95.0 | J |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 | kJ/m² |
| -10°C | ISO 180/1A | 5.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 3.0mm | UL 94 | V-2 | |
| Burning wire flammability index | 1.0mm | IEC 60695-2-12 | 750 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ISO 178 | 75.0 | Mpa | |
| Bending modulus | ISO 178 | 2000 | Mpa | |
| 50.0mmSpan | ASTM D790 | 1960 | Mpa | |
| Tensile strain | Break | ISO 527-2/50 | >150 | % |
| elongation | Break | ASTM D638 | 140 | % |
| Tensile strain | Yield | ISO 527-2/5 | 5.0 | % |
| elongation | Yield | ASTM D638 | 5.0 | % |
| tensile strength | Break | ISO 527-2/50 | 56.0 | Mpa |
| Break | ASTM D638 | 56.0 | Mpa | |
| Yield | ISO 527-2/50 | 55.0 | Mpa | |
| bending strength | Yield,50.0mmSpan | ASTM D790 | 84.0 | Mpa |
| Tensile modulus | ASTM D638 | 1880 | Mpa | |
| ISO 527-2/1 | 2000 | Mpa | ||
| tensile strength | Yield | ASTM D638 | 55.0 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C |
| TD:-40to40°C | ASTME831 | 1.1E-04 | cm/cm/°C | |
| MD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C | |
| MD:-40to40°C | ASTME831 | 1.1E-04 | cm/cm/°C | |
| Ball Pressure Test | 105°C | IEC 60695-10-2 | Pass | |
| Vicat softening temperature | ISO 306/B120 | 115 | °C | |
| ASTM D15259 | 115 | °C | ||
| Hot deformation temperature | 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 99.0 | °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | 90.0 | °C | |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 96.0 | °C | |
| thermal conductivity | ISO 8302 | 0.23 | W/m/K | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 265°C/2.16kg | ASTM D1238 | 12 | g/10min |
| Melt Volume Flow Rate (MVR) | 265°C/2.16kg | ISO 1133 | 12.0 | cm3/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 | % |
| TD:3.20mm | Internal Method | 0.50-0.70 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ASTM D257 | >1.0E+15 | ohms | |
| Volume resistivity | ASTM D257 | >1.0E+15 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD,10Sec | ASTM D2240 | 76 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.