POM DURACON® ES-5 JAPAN POLYPLASTIC

199
  • Unit Price:US$ 3,770 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    50.4MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High temperature resistancewear resistant
  • Application Areas:household electrical appliancesAutomotive Applications
  • Color:--
  • Grade:Special level

Material Certification

UL

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest Result
densityISO 11831.41 g/cm³
melt mass-flow rateISO 11339.0 g/10min
Melt volume flow rateISO 11338.00 cm3/10min
Shrinkage rateISO 294-42.0 %
Shrinkage rateISO 294-42.0 %
Water absorption rateISO 621.3 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessISO 2039-290
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Supplementary InformationTest ConditionTest MethodTest Result
ColorNumberCD3501
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-22850 Mpa
tensile strength ISO 527-249.0 Mpa
Tensile strainISO 527-27.5 %
Flexural modulusISO 1782600 Mpa
bending strengthISO 17884.0 Mpa
coefficient of frictionJISK72180.43
coefficient of frictionJISK72180.47
Wear factorJISK7218<1.0 10^-8mm³/N·m
Wear factorJISK721880 10^-8mm³/N·m
Wear factorJISK72181200 10^-8mm³/N·m
Wear factorJISK72184000 10^-8mm³/N·m
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 179/1eA3.0 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
Surface Resistivity内部方法5E+02 ohms
Volume resistivity内部方法1E+02 ohms·cm
Thermal performanceTest ConditionTest MethodTest Result
Linear coefficient of thermal expansion内部方法1.1E-04 cm/cm/°C
Linear coefficient of thermal expansion内部方法1.1E-04 cm/cm/°C
Heat distortion temperatureISO 75-2/A109 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.