PA66 Zytel® FR95G25V0NH NC010 DUPONT BELGIUM
251
- Unit Price:US$ 9,396 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|Filler: Glass fiber reinforced material|25% filler by weight
- Application Areas:Automotive Applications|Electrical applications|currency|Industrial applications
- Color:--
- Grade:High liquidity level
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 35 kJ/m² |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 0.75mm | IEC 60695-11-10,-20 | V-0 |
1.5mm | IEC 60695-11-10,-20 | V-0 | |
1.5mm | UL 94 | V-0 | |
0.75mm | UL 94 | V-0 | |
Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
Extreme Oxygen Index | ISO 4589-2 | 32 % | |
FMVSS flammability | FMVSS302 | B |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ISO 178 | 185 Mpa | |
Bending modulus | ISO 178 | 9000 Mpa | |
Tensile strain | Break | ISO 527-2 | 2.2 % |
tensile strength | Break | ISO 527-2 | 109 Mpa |
Tensile modulus | ISO 527-2 | 8900 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
TemperatureIndex | TensileStrength,5000hr | IEC 60216 | 190 °C |
TensileStrength,20000hr | IEC 60216 | 160 °C | |
RTI Elec | 3.0mm | UL 746 | 160 °C |
1.5mm | UL 746 | 160 °C | |
0.75mm | UL 746 | 160 °C | |
0.40mm | UL 746 | 160 °C | |
Melting temperature | ISO 11357-3 | 267 °C | |
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 233 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Top out temperature | 210 °C | ||
Shrinkage rate | TD | ISO 294-4 | 0.60 % |
Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 4.0 % |
Shrinkage rate | MD | ISO 294-4 | 0.10 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
Dielectric strength | IEC 60243-1 | 37 KV/mm | |
Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
Surface resistivity | IEC 60093 | -- ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.