PA66 Leona™ FR370 ASAHI JAPAN
194
- Unit Price:US$ 4,764 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :Huangpu port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Dongguan East Asia Plastic Co., Ltd.
+86 1380********View
1925********View
For more details, please contact the supplier!
Material Description
- Material Properties:Flame retardant|Halogen-free
- Application Areas:Laptop case|switch|Electrical components|Electronic field|Electrical field
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | 难燃性 | |||
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | 干 | ASTM D-2863 | 36 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of simply supported beam without notch | ISO 179 | 58 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.75mm | UL 94 | V-0 | |
| Burning wire flammability index | 3.0mm | IEC 60695-2-12 | 960 | °C |
| Extreme Oxygen Index | ASTM D2863 | 36 | % | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 湿 | 2.3 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | 23°C | ISO 178 | 3600 | Mpa |
| ASTM D790 | 3300 | Mpa | ||
| Tensile strain | Break,23°C | ISO 527-2 | 15 | % |
| elongation | Break | ASTM D638 | 7.0 | % |
| Tensile strain | Yield,23°C | ISO 527-2 | 4.5 | % |
| tensile strength | Break,23°C | ISO 527-2 | 80.0 | Mpa |
| Yield,23°C | ISO 527-2 | 83.0 | Mpa | |
| ASTM D638 | 83.0 | Mpa | ||
| Tensile modulus | 23°C | ISO 527-2 | 3600 | Mpa |
| bending strength | ASTM D790/ISO 178 | 127 | kg·cm/cm(J/M)ft·lb/in | |
| Bending modulus | ASTM D790/ISO 178 | 3330 | kg·cm/cm(J/M)ft·lb/in | |
| tensile strength | ASTM D638/ISO 527 | 83.4 | kg/cm²(MPa)[Lb/in²] | |
| Elongation at Break | ASTM D638/ISO 527 | 7 | % | |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 29 | kg·cm/cm(J/M)ft·lb/in | |
| bending strength | ASTM D790 | 128 | Mpa | |
| 23°C | ISO 178 | 124 | Mpa | |
| Taber abraser | 1000Cycles | ASTM D1044 | -- | mg |
| tensile strength | 干(湿) | ASTM D-638 | 83(58) | Mpa |
| Rockwell hardness | 干(湿) | ASTM D-785 | 120(110) | R scale |
| Elongation at Break | 干(湿) | ASTM D-638 | 7(70) | % |
| Impact strength of cantilever beam gap | 干(湿) | ASTM D-256 | 29(58) | J/m |
| bending strength | 干(湿) | ASTM D-790 | 128(56) | Mpa |
| flexural coefficient | 干(湿) | ASTM D-790 | 3.3(1.3) | GPa |
| Rockwell hardness | 干(湿) | ASTM D-785 | 85(55) | M Scale |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 8 | mm/mm.℃ | |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 240 | ℃(℉) |
| Combustibility (rate) | UL 94 | V-0 | ||
| Hot deformation temperature | 1.82MPa,干 | ASTM D-648 | 80 | °C |
| UL flame retardant rating | 干 | UL 94 | V-0 | |
| Linear coefficient of thermal expansion | 干 | ASTM D-696 | 7 | |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 240 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 239 | °C | |
| 1.8MPa,Unannealed | ASTM D648 | 80.0 | °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 78.0 | °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7E-05 | cm/cm/°C |
| Hot deformation temperature | 0.46MPa,干 | ASTM D-648 | 240 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | -- | % |
| Saturation,23°C | -- | % | ||
| Shrinkage rate | MD | Internal Method | 0.90-1.6 | % |
| Water absorption rate | ASTM D570/ISO 62 | 2.3 | % | |
| Shrinkage rate | ASTM D955 | 0.9-1.6 | % | |
| density | ASTM D792/ISO 1183 | 1.16 | ||
| Shrinkage rate | 干 | 旭化成方法 | 0.9-1.6 | % |
| Wear factor | 湿 | ASTM D-1044 | 7 | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | ASTM D257/IEC 60093 | 10*10 | Ω.cm | |
| Surface resistivity | ASTM D257 | 1E+13 | ohms | |
| IEC 60093 | 1E+13 | ohms | ||
| Volume resistivity | ASTM D257 | 1E+14 | ohms·cm | |
| 23°C | IEC 60093 | 1E+14 | ohms·cm | |
| Dielectric strength | ASTM D149 | 22 | KV/mm | |
| IEC 60243-1 | 22 | KV/mm | ||
| Compared to the anti leakage trace index | 3.00mm | IEC 60112 | PLC 0 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Sale | ASTM D785 | 85 | |
| R-Sale | ASTM D785 | 120 | ||
| M-Sale | ISO 2039-2 | 85 | ||
| R-Sale | ISO 2039-2 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.