Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Weather resistant grade
Technical Data Sheet
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | 横向Flow:100%Strain | ASTM D412 | 3.10 Mpa |
Flow:100%Strain | ASTM D412 | 3.50 Mpa | |
横向Flow:100%Strain | ISO 37 | 3.10 Mpa | |
Flow:100%Strain | ISO 37 | 3.50 Mpa | |
Break | ASTM D412 | 6.60 Mpa | |
Flow:Break | ASTM D412 | 6.00 Mpa | |
Break | ISO 37 | 6.60 Mpa | |
Flow:Break | ISO 37 | 6.00 Mpa | |
elongation | Break | ASTM D412 | 490 % |
Flow:Break | ASTM D412 | 410 % | |
Break | ISO 37 | 490 % | |
Flow:Break | ISO 37 | 410 % | |
tear strength | 横向Flow | ASTM D624 | 33.3 kN/m |
横向Flow | ISO 34-1 | 33 kN/m | |
Permanent compression deformation | 23°C,22hr | ASTM D395 | 24 % |
70°C,22hr | ASTM D395 | 36 % | |
125°C,70hr | ASTM D395 | 52 % | |
23°C,22hr | ISO 815 | 24 % | |
70°C,22hr | ISO 815 | 36 % | |
125°C,70hr | ISO 815 | 52 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ShoreA,5Sec,挤塑 | ISO 868 | 74 |
ShoreA,5Sec,Injection | ISO 868 | 76 | |
ShoreA,5Sec,挤塑 | ASTM D2240 | 74 | |
ShoreA,5Sec,Injection | ASTM D2240 | 76 |
aging | Test Condition | Test Method | Test Result |
---|---|---|---|
Change rate of tensile strength in air | 135°C,1000hr,Across Flow | ASTM D573 | -12 % |
100%Strain,135°C,1000hr,Across Flow | ASTM D573 | 5.0 % | |
150°C,168hr,Across Flow | ASTM D573 | -22 % | |
100%Strain,150°C,168hr,Across Flow | ASTM D573 | 2.0 % | |
135°C,1000hr,Across Flow | ISO 188 | -12 % | |
100%Strain135°C,1000hr,Across Flow | ISO 188 | 5.0 % | |
150°C,168hr,Across Flow | ISO 188 | -22 % | |
100%Strain150°C,168hr,Across Flow | ISO 188 | 2.0 % | |
Change rate of ultimate elongation in air | 135°C,1000hr,Across Flow | ASTM D573 | -16 % |
150°C,168hr,Across Flow | ASTM D573 | -29 % | |
Tensile stress change rate | 135°C,1000hr,Break | ISO 188 | -16 % |
150°C,168hr,Break | ISO 188 | -29 % | |
Change rate of hardness (Shore) in the air | ShoreA,135°C,1000hr | ASTM D573 | 3.0 |
ShoreA,150°C,168hr | ASTM D573 | 1.0 | |
ShoreA,135°C,1000hr | ISO 188 | 3.0 | |
ShoreA,150°C,168hr | ISO 188 | 1.0 | |
Volume change | 125°C,70hr,在IRM903油中 | ASTM D471 | 74 % |
125°C,70hr,在IRM903油中 | ISO 1817 | 74 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Apparent viscosity | 200°C,剪切,毛细管法, @206/s | ISO 11443 | 220 Pa·s |
200°C,剪切,毛细管法, @206/s | ASTM D3835 | 220 Pa·s |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.