AS(SAN) Luran® 368R INEOS STYRO THAILAND
410
- Unit Price:US$ 2,305 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:65MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:transparent|Good stability
- Application Areas:Monitor|Pen|Household goods|Electrical appliances|Toothbrush handle
- Color:--
- Grade:Injection grade
Technical Data Sheet
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Refractive index | ISO 489 | 1.569 | |
transmissivity | 550nm | ASTM D1003 | >89.0 % |
turbidity | ASTM D1003 | <1.0 % |
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179 | 18 kJ/m² |
23°C | ISO 179 | 18 kJ/m² |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 3700 Mpa | |
tensile strength | Yield,23°C | ISO 527-2 | 75.0 Mpa |
Tensile strain | Break,23°C | ISO 527-2 | 3.0 % |
Tensile creep modulus | 1hr | ISO 899-1 | 3500 Mpa |
1000hr | ISO 899-1 | 2800 Mpa | |
bending strength | ISO 178 | 125 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Vicat softening temperature | ISO 306/B50 | 106 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 7E-05 cm/cm/°C |
thermal conductivity | DIN 52612 | 0.17 W/m/K | |
Hot deformation temperature | 0.45MPa,Annealed | ISO 75-2/B | 100 °C |
1.8MPa,Annealed | ISO 75-2/A | 88.0 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Apparent density | 0.65 g/cm³ | ||
Melt Volume Flow Rate (MVR) | 220°C/10.0kg | ISO 1133 | 10.0 cm3/10min |
Shrinkage rate | ISO 294-4 | 0.30-0.70 % | |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface resistivity | IEC 60093 | >1.0E+15 ohms | |
Volume resistivity | IEC 60093 | 1E+16 ohms·cm | |
Dielectric constant | 100Hz | IEC 60250 | 3.00 |
Dissipation factor | 100Hz | IEC 60250 | 4E-03 |
1MHz | IEC 60250 | 7E-03 |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | M-Scale | 83 | |
Ball Pressure Test | ISO 2039-1 | 165 Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.