PPO/PA NORYL GTX™ GTX675 SABIC INNOVATIVE US
500
- Unit Price:US$ 4,990 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:65MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility|dimensional stability |High temperature resistance|Hydrolysis resistance
- Application Areas:Electrical applications|Industrial machinery
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 5.00 | J |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 12 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | -- | ISO 527-2/1 | 2670 | Mpa |
| tensile strength | Yield3 | ASTM D638 | 65.0 | Mpa |
| Yield | ISO 527-2/50 | 66.0 | Mpa | |
| Tensile modulus | --2 | ASTM D638 | 2420 | Mpa |
| bending strength | Yield,50.0mmSpan4 | ASTM D790 | 100 | Mpa |
| --5,6 | ISO 178 | 103 | Mpa | |
| Bending modulus | --5 | ISO 178 | 2470 | Mpa |
| 50.0mmSpan4 | ASTM D790 | 2520 | Mpa | |
| elongation | Break | ISO 527-2/50 | 7.1 | % |
| Break3 | ASTM D638 | 6.1 | % | |
| tensile strength | Break3 | ASTM D638 | 63.0 | Mpa |
| Break | ISO 527-2/50 | 64.0 | Mpa | |
| elongation | Yield3 | ASTM D638 | 3.8 | % |
| Yield | ISO 527-2/50 | 4.0 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | 通过 | |
| Vicat softening temperature | -- | ISO 306/B120 | 198 | °C |
| -- | ASTMD152510 | 197 | °C | |
| Hot deformation temperature | 0.45MPa,Unannealed,64.0mmSpan9 | ISO 75-2/Bf | 184 | °C |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 187 | °C | |
| Linear coefficient of thermal expansion | TD:23to60°C | ISO 11359-2 | 8.6E-05 | cm/cm/°C |
| TD:-40to40°C | ASTME831 | 7.8E-05 | cm/cm/°C | |
| MD:23to60°C | ISO 11359-2 | 8.1E-05 | cm/cm/°C | |
| MD:-40to40°C | ASTME831 | 7.6E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.40 | % |
| Saturation,23°C | ISO 62 | 4.0 | % | |
| Shrinkage rate | MD:3.20mm | Internal Method | 1.3-1.5 | % |
| Melt Volume Flow Rate (MVR) | 300°C/5.0kg | ISO 1133 | 7.00 | cm3/10min |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 7.8 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | Internal Method | 1.0E+3-1.0E+4 | ohms·cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.