plas

PA66 Zytel®  XT70G35HSL BK044A DUPONT USA

223
  • Unit Price:US$ 4,917 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Fatigue resistanceHigh temperature resistanceFiller: Glass fiber reinforced material35% filler by weight35% filler by weight
  • Application Areas:Automotive sector
  • Color:--
  • Grade:--

Technical Data Sheet

mechanical propertiesTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap-30°CISO 180/1A10 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A12 kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU80 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU90 kJ/m²
Charpy Notched Impact Strength-30°CISO 179/1eA10 kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA15 kJ/m²
Tensile modulus23°CISO 527-211200 Mpa
Elongation at Break23°CISO 527-23.20 %
tensile strength23°CISO 527-2210 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPaUnannealedISO 75-2/Bf261 °C
Hot deformation temperature1.80MPaAnnealedISO 75-2/Af252 °C
Linear coefficient of thermal expansionTDISO 11359-21E-04 cm/cm/°C
Linear coefficient of thermal expansionMDISO 11359-22E-05 cm/cm/°C
Vicat softening temperatureMelting TemperatureISO 11357-3262 °C
Vicat softening temperatureISO 306/B50255 °C
Vicat softening temperature玻璃转化温度ISO 11357-280 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateTD2.0mmISO 294-41.10 %
Shrinkage rateMD2.0mmISO 294-40.30 %
densityISO 11831.41 g/cm³
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor相对漏电起痕指数IEC 60112400 V
Dielectric strengthIEC 60243-133 KV/mm
Volume resistivityIEC 600931E+13 Ω.cm
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessISO 2039-2125 R
Rockwell hardnessISO 2039-2105 M(Scale)
flame retardant performanceTest ConditionTest MethodTest Result
Extreme Oxygen IndexISO 4589-224 %
UL flame retardant ratingUL -94HB 3.00mm
UL flame retardant ratingUL -94HB 1.50mm
UL flame retardant ratingUL -94HB 0.71mm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.