PA12 VESTAMID® E62S3 EVONIK GERMANY
93
- Unit Price:US$ 26,800 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Plastic bag
- Supply Quantity:2MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
Shenzhen Benia New Materials Technology Co., Ltd.
+86 1892********View
oswa********View
For more details, please contact the supplier!
Material Description
- Material Properties:Easy to process|Low temperature impact resistance|Photostability|Antisolvent|High elasticity|low density
- Application Areas:Engine parts|Conveyor accessories|sporting goods
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23℃23°C | ISO 179/1eU | No Break | |
| -30℃-30°C | ISO 179/1eU | No Break | ||
| Charpy Notched Impact Strength | 23℃,Partial Break73°F, Partial Break | ISO 179/1eA | 120 | kJ/m² |
| -30℃,Complete Break-22°F, Complete Break | ISO 179/1eA | 8 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile creep modulus | 1000 hr1000 hr | ISO 899-1 | 200 | Mpa |
| Tensile strain | BreakBreak | ISO 527-2 | > 200 | % |
| tensile strength | 50% Strain50% Strain | ISO 527-2 | 23 | Mpa |
| ---- | ISO 527-2 | 42 | Mpa | |
| Tensile modulus | ISO 527-2 | 370 | Mpa | |
| Shore hardness | Shore DShore D | ISO 868 | 62 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:23~55℃MD:23 to 55℃ | ISO 11359-2 | 0.00020 | 1/℃ |
| TD:23~55℃TD:23 to 55℃ | ISO 11359-2 | 0.00020 | 1/℃ | |
| Vicat softening temperature | ---- | ISO 306/B | 110 | °C |
| ---- | ISO 306/A | 165 | °C | |
| Hot deformation temperature | 0.45 MPa,Unannealed0.45 MPa,Unannealed | ISO 75-2/B | 100 | °C |
| 1.8 MPa,Unannealed1.8 MPa,Unannealed | ISO 75-2/A | 45 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Stickiness | ISO 307 | 190 | cm³/g | |
| Water absorption rate | Saturation,23℃Saturation,23℃ | ISO 62 | 1.1 | % |
| Shrinkage rate | MDFlow | ISO 294-4 | 0.60 - 1.1 | % |
| TDAcross Flow | ISO 294-4 | 0.90 - 1.4 | % | |
| density | ISO 1183 | 1.03 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Relative permittivity | 23℃,100 Hz23°C, 100 Hz | IEC 60250 | 9 | |
| 23℃,1 MHz23°C, 1 MHz | IEC 60250 | 4 | ||
| Dissipation factor | 23℃,100 Hz23°C, 100 Hz | IEC 60250 | 0.1 | |
| Dielectric strength | IEC 60243-1 | 39 | KV/mm | |
| Volume resistivity | IEC 60093 | 1000000000000 | ohms·cm | |
| Surface resistivity | IEC 60093 | 100000000000000 | ohms | |
| Dissipation factor | 23℃,1 MHz23°C, 1 MHz | IEC 60250 | 0.12 | |
| Compared to the anti leakage trace index | Solution ASolution A | IEC 60112 | PLC 0 | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| 1.60 mm??1.6 mm | 1.60mm | UL 94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.